- 专利标题: Method for producing impact-resistant polyester resin compositions
- 专利标题(中): 维多利亚·赫斯特伦·施拉格特
-
申请号: EP91309414.0申请日: 1991-10-14
-
公开(公告)号: EP0480769A2公开(公告)日: 1992-04-15
- 发明人: Ohmae, Tadayuki , Toyoshima, Yoshiki , Mashita, Kentaro , Yamaguchi, Noboru , Chikanari, Kenzo
- 申请人: SUMITOMO CHEMICAL COMPANY, LIMITED
- 申请人地址: 5-33, Kitahama 4-chome Chuo-ku Osaka JP
- 专利权人: SUMITOMO CHEMICAL COMPANY, LIMITED
- 当前专利权人: SUMITOMO CHEMICAL COMPANY, LIMITED
- 当前专利权人地址: 5-33, Kitahama 4-chome Chuo-ku Osaka JP
- 代理机构: Cresswell, Thomas Anthony
- 优先权: JP272281/90 19901012
- 主分类号: C08L67/02
- IPC分类号: C08L67/02 ; C08L23/08 ; C08L51/06 ; C08J3/00
摘要:
A saturated polyester resin composition excellent in impact resistance is prepared by melt kneading (A) 30-58 parts by weight of a saturated polyester resin, (B) 42-70 parts by weight of an epoxy group-containing ethylene copolymer comprising (a) 50-99% by weight of ethylene unit, (b) 0.1-30% by weight of unsaturated carboxylic acid glycidyl ester unit or unsaturated glycidyl ether unit, and (c) 0-49% by weight of ethylenically unsaturated ester compound unit, (C) 0.01-20 parts by weight of a polyfunctional compound containing at least two specific functional groups of amino groups, carboxyl groups, carboxylic acid anhydride groups, hydroxyl groups or
unit (wherein X and Y are both oxygen atoms or sulfur atoms or one of them is an oxygen atom and another is a sulfur atom) and (D) 0-30 parts by weight of a block copolyether ester elastomer, the amounts of (C) and (D) being based on 100 parts by weight of (A) plus (B), thereby to obtain a former-stage composition (I) and furthermore melt kneading the resulting composition (I) with (E) 50-1000 parts by weight of a saturated polyester resin and (F) 0-30 parts by weight of a block copolyether ester elastomer at a later-stage.
unit (wherein X and Y are both oxygen atoms or sulfur atoms or one of them is an oxygen atom and another is a sulfur atom) and (D) 0-30 parts by weight of a block copolyether ester elastomer, the amounts of (C) and (D) being based on 100 parts by weight of (A) plus (B), thereby to obtain a former-stage composition (I) and furthermore melt kneading the resulting composition (I) with (E) 50-1000 parts by weight of a saturated polyester resin and (F) 0-30 parts by weight of a block copolyether ester elastomer at a later-stage.