- 专利标题: PROCESS FOR RECOVERY OF NICKEL AND COBALT BY HEAP LEACHING OF LOW GRADE NICKEL OR COBALT CONTAINING MATERIAL
- 专利标题(中): 一种获得镍和钴的堆浸低品位镍或钴材料
-
申请号: EP04737564.7申请日: 2004-07-13
-
公开(公告)号: EP1644541B1公开(公告)日: 2011-08-24
- 发明人: MILLER, Geoffrey, William , LIU, Houyuan
- 申请人: BHP Billiton SSM Development Pty Ltd
- 申请人地址: Level 33, Central Park 152-158 St Georges Terrace Perth, WA 6000 AU
- 专利权人: BHP Billiton SSM Development Pty Ltd
- 当前专利权人: BHP Billiton SSM Development Pty Ltd
- 当前专利权人地址: Level 33, Central Park 152-158 St Georges Terrace Perth, WA 6000 AU
- 代理机构: Moy, David
- 优先权: AU2003903632 20030714
- 国际公布: WO2005005671 20050120
- 主分类号: C22B3/06
- IPC分类号: C22B3/06 ; C22B3/04 ; C22B3/08 ; C22B3/10 ; C22B23/00 ; B03B5/00 ; B03B7/00
摘要:
A process for the recovery of nickel and cobalt from laterite ores, the process including the steps of: a) beneficiating the ore to separate it into a beneficiated upgraded ore fraction and a coarse, siliceous low grade rejects fraction which is substantially free from fines and clay materials; b) separately processing the upgraded ore fraction for the recovery of nickel and cobalt; and c) subjecting the low grade rejects fraction to a heap leach process with an acid supplemented solution to create a heap leachate for further nickel and cobalt recovery processing.