发明授权
- 专利标题: Low thermal expansion Ni-base superalloy
- 专利标题(中): 低热膨胀Ni基高温合金
-
申请号: EP11008616.2申请日: 2007-06-13
-
公开(公告)号: EP2418295B1公开(公告)日: 2017-10-11
- 发明人: Hamano, Shuji , Ueta, Shigeki , Yamamoto, Ryuichi , Kadoya, Yoshikuni , Nakano, Takashi , Nishimoto, Shin
- 申请人: Daido Tokushuko Kabushiki Kaisha , Mitsubishi Heavy Industries, Ltd.
- 申请人地址: 1-10 Higashisakura 1-chome Higashi-ku Nagoya Aichi JP
- 专利权人: Daido Tokushuko Kabushiki Kaisha,Mitsubishi Heavy Industries, Ltd.
- 当前专利权人: Daido Tokushuko Kabushiki Kaisha,Mitsubishi Heavy Industries, Ltd.
- 当前专利权人地址: 1-10 Higashisakura 1-chome Higashi-ku Nagoya Aichi JP
- 代理机构: Diehl & Partner GbR
- 优先权: JP2006163969 20060613
- 主分类号: C22C19/05
- IPC分类号: C22C19/05
摘要:
The present invention relates to a low thermal expansion Ni-base superalloy containing, in terms of mass %, C: 0.15% or less; Si: 1% or less; Mn: 1% or less; Cr: 5% or more but less than 20%; at least one of Mo, W and Re, in which Mo + 1/2(W + Re) is 5% or more but less than 20%; W: 10% or less; Al: 0.1 to 2.5%; Ti: 0.10 to 0.95%; Nb + 1/2Ta: 1.5% or less; B: 0.001 to 0.02%; Zr: 0.001 to 0.2%; Fe: 4.0% or less; and a balance of inevitable impurities and Ni, in which the total amount of Al, Ti, Nb and Ta is 2.0 to 6.5% in terms of atomic %. The low thermal expansion Ni-base superalloy of the present invention has a thermal expansion coefficient almost equal to that of 12 Cr ferritic steel, excellent high temperature strength, excellent corrosion and oxidation resistance, good hot-workability, and excellent weldability.