EP3045142A1 ENDODONTIC INSTRUMENTS AND METHODS OF MANUFACTURIN THEREOF
有权
内罗毕仪器公司在维多利亚州ZER HERSTELLUNG DAVON
- 专利标题: ENDODONTIC INSTRUMENTS AND METHODS OF MANUFACTURIN THEREOF
- 专利标题(中): 内罗毕仪器公司在维多利亚州ZER HERSTELLUNG DAVON
-
申请号: EP16156160.0申请日: 2012-11-16
-
公开(公告)号: EP3045142A1公开(公告)日: 2016-07-20
- 发明人: AMMON, Dan , SHOTTON, Vincent , GAO, Yong , MAXWELL, Randall
- 申请人: Dentsply International Inc.
- 申请人地址: 570 West College Avenue York, PA 17401-3880 US
- 专利权人: Dentsply International Inc.
- 当前专利权人: Dentsply International Inc.
- 当前专利权人地址: 570 West College Avenue York, PA 17401-3880 US
- 代理机构: Hartz, Nikolai
- 优先权: US201113300506 20111118
- 主分类号: A61C5/02
- IPC分类号: A61C5/02 ; C21D6/00 ; C21D9/00
摘要:
A method for manufacturing a non-superelastic file comprising the steps of:
(i) providing a superelastic file having an austenite finish temperature; and
(ii) heating at least a portion of the superelastic file to a temperature from 300 °C to 600 °C for a period of time from 5 minu tes to 120 minutes to alter the austenite finish temperature thereby forming the non-superelastic file; wherein the altered austenite finish temperature of the non-superelastic file is from 20°C to 40°C;
further comprising the step of
(iii) cooling the portion of the non- superelastic file, and
(iv) heating at least a portion of the cooled non-superelastic file to a temperature from 350°C to 600°C for a time period from 3 minutes to 30 minutes to shape-set the portion of the shaft thereby forming a shape-set non-superelastic nonlinear file.
(i) providing a superelastic file having an austenite finish temperature; and
(ii) heating at least a portion of the superelastic file to a temperature from 300 °C to 600 °C for a period of time from 5 minu tes to 120 minutes to alter the austenite finish temperature thereby forming the non-superelastic file; wherein the altered austenite finish temperature of the non-superelastic file is from 20°C to 40°C;
further comprising the step of
(iii) cooling the portion of the non- superelastic file, and
(iv) heating at least a portion of the cooled non-superelastic file to a temperature from 350°C to 600°C for a time period from 3 minutes to 30 minutes to shape-set the portion of the shaft thereby forming a shape-set non-superelastic nonlinear file.