- 专利标题: METAL-CARBON FIBER REINFORCED PLASTIC MATERIAL COMPOSITE AND PRODUCTION METHOD FOR METAL-CARBON FIBER REINFORCED PLASTIC MATERIAL COMPOSITE
-
申请号: EP19818808.8申请日: 2019-06-14
-
公开(公告)号: EP3808557A1公开(公告)日: 2021-04-21
- 发明人: KAWAMURA, Yasuaki , UEDA , Kohei , KOORI, Masumi
- 申请人: NIPPON STEEL CORPORATION
- 申请人地址: JP Chiyoda-ku Tokyo 100-8071 6-1, Marunouchi 2-chome
- 代理机构: Vossius & Partner Patentanwälte Rechtsanwälte mbB
- 优先权: JP2018113340 20180614
- 国际公布: WO2019240283 20191219
- 主分类号: B32B15/08
- IPC分类号: B32B15/08 ; B32B27/00 ; B32B27/38
摘要:
To provide a metal-carbon fiber reinforced plastic material (CFRP) composite that has excellent adhesion and adhesion durability at a member interface and a method of producing a metal-CFRP composite.
The metal-CFRP composite according to the present invention includes: a metal member; a CFRP layer; and one or two layers of coating layers provided between the metal member and the CFRP layer. In the case where the coating layer consists of one layer, the coating layer is a coating layer containing an isocyanate group, and the matrix resin contains a phenoxy resin as a main component thereof, contains an epoxy group, and has bonds represented in (a structural formula 1) in the vicinity of an interface between the CFRP layer and the coating layer. In the case where the coating layer consists of two layers, the first coating layer that is located on the metal member side is a coating layer containing an isocyanate group, and the second coating layer that is located on the CFRP layer side is a coating layer that contains an epoxy resin as a main component thereof, and has bonds represented in (a structural formula 1) in the vicinity of an interface between the first coating layer and the second coating layer.
The metal-CFRP composite according to the present invention includes: a metal member; a CFRP layer; and one or two layers of coating layers provided between the metal member and the CFRP layer. In the case where the coating layer consists of one layer, the coating layer is a coating layer containing an isocyanate group, and the matrix resin contains a phenoxy resin as a main component thereof, contains an epoxy group, and has bonds represented in (a structural formula 1) in the vicinity of an interface between the CFRP layer and the coating layer. In the case where the coating layer consists of two layers, the first coating layer that is located on the metal member side is a coating layer containing an isocyanate group, and the second coating layer that is located on the CFRP layer side is a coating layer that contains an epoxy resin as a main component thereof, and has bonds represented in (a structural formula 1) in the vicinity of an interface between the first coating layer and the second coating layer.