Method for preparing pearlescent pigment from ilmenite hydrochloric acid acidolysis solution by co-extraction
Abstract:
A preparation method of pearlescent pigment coating materials is provided. The method of the present invention lies in that titanium-iron ions in ilmenites are dissolved by using a hydrochloric acid at a certain temperature and pressure, and then ferrous chloride in the acidolysis solution is precipitated by adding hydrogen chloride gas, the remaining titanium-iron ions are separated from other colored ions by means of co-extraction using an extractant upon oxidation, and an enriched titanium oxydichloride solution and ferrous hydrous oxide are obtained by employing a fractional back extraction and enrichment method, the titanium oxydichloride solution can be used for mica-titanium based pearlescent pigment coating materials, and can also be used for preparing titanium dioxide; and the acidified ferrous hydrous oxide and the oxidized ferrous chloride can be used as iron based pearlescent pigment coating materials or used for preparing iron oxide pigments.
Information query
Patent Agency Ranking
0/0