The present disclosure relates to a carbon black dispersion solution comprising carbon black, a dispersion medium, and partially hydrogenated nitrile rubber having a residual double bond (RDB) value of 0.5% by weight to 40% by weight calculated according to the following Mathematical Formula 1, wherein dispersed particle diameters of the carbon black have particle size distribution D50 of 0.1 μm to 2 μm, a method for preparing the same, and methods for preparing electrode slurry and an electrode using the same.