Braze alloys for joining or repairing ceramic matrix composite (CMC) components
Abstract:
A braze alloy for joining or repairing ceramic matrix composite (CMC) components comprises a braze composition including silicon at a concentration from about 48 at. % to about 66 at. %, titanium at a concentration from about 1 at. % to about 35 at. %, and an additional element selected from aluminum, cobalt, vanadium, nickel, and chromium. The braze composition comprises a melting temperature of less than 1300° C.