- 专利标题: Silver brazing material and joining method using the silver brazing material
-
申请号: US17048086申请日: 2018-10-24
-
公开(公告)号: US11638973B2公开(公告)日: 2023-05-02
- 发明人: Takaomi Kishimoto , Masahiro Takahashi , Takashi Terui , Kotaro Matsu
- 申请人: TANAKA KIKINZOKU KOGYO K.K. , TOKYO BRAZE CO., LTD.
- 申请人地址: JP Tokyo; JP Tokyo
- 专利权人: TANAKA KIKINZOKU KOGYO K.K.,TOKYO BRAZE CO., LTD.
- 当前专利权人: TANAKA KIKINZOKU KOGYO K.K.,TOKYO BRAZE CO., LTD.
- 当前专利权人地址: JP Tokyo; JP Tokyo
- 代理机构: Foley & Lardner LLP
- 优先权: JPJP2018-082005 20180423
- 国际申请: PCT/JP2018/039405 WO 20181024
- 国际公布: WO2019/207823 WO 20191031
- 主分类号: B23K35/30
- IPC分类号: B23K35/30 ; B23K1/00 ; B23K1/19 ; B23K101/20 ; B23K103/12 ; B23K1/008 ; B23K31/02
摘要:
A silver brazing material containing silver, copper, zinc, manganese, nickel, and tin as indispensable constituent elements. The silver brazing material includes 35 mass % or more and 45 mass % or less silver, 18 mass % or more and 28 mass % or less zinc, 2 mass % or more and 6 mass % or less manganese, 1.5 mass % or more and 6 mass % or less nickel, and 0.5 mass % or more and 5 mass % or less tin, with the balance being copper impurities. Within these compositional ranges, a predetermined relation is set between the manganese content and the nickel content, whereby the silver brazing material can be provided with excellent characteristics also in terms of processability or wettability. In the silver brazing material of the present invention, the silver content is reduced, and also melting point reduction and the narrowing of the temperature difference between solidus temperature and liquidus temperature are attempted.