Method for preparing calcium oxide using a multistage suspension preheater kiln
Abstract:
The disclosure discloses a method for preparing calcium oxide using multistage suspension preheater kiln. The steps of the method are: (1) the limestone powder is fed to the multistage suspension preheater kiln for preheating to 800° C. to 900° C.; (2) A preheated material is fed to a decomposition furnace, and calcined at 900° C. to 1100° C. for 25 s to 35 s; (3) A calcined material is fed to a rotary kiln, and calcined at 1100° C. to 1300° C. for 25 to 35 minutes, and finally cooled to obtain calcium oxide.