US20090288747A1 Metal Cord, Rubber-Cord Complex and Pneumatic Tire Using the Same
审中-公开
金属线,橡胶线复合体和使用其的气动轮胎
- 专利标题: Metal Cord, Rubber-Cord Complex and Pneumatic Tire Using the Same
- 专利标题(中): 金属线,橡胶线复合体和使用其的气动轮胎
-
申请号: US12085347申请日: 2006-11-30
-
公开(公告)号: US20090288747A1公开(公告)日: 2009-11-26
- 发明人: Shinichi Miyazaki , Junichi Kodama , Yasuo Sakai , Keisuke Aramaki , Yuichi Sano , Kenichi Okamoto
- 申请人: Shinichi Miyazaki , Junichi Kodama , Yasuo Sakai , Keisuke Aramaki , Yuichi Sano , Kenichi Okamoto
- 申请人地址: JP Kobe-shi JP Tokyo JP Itami-shi
- 专利权人: Sumitomo Rubber Industriesm, Ltd.,Nippon Steel Corporation,Sumitomo (SEI) Steel Wire Corp.
- 当前专利权人: Sumitomo Rubber Industriesm, Ltd.,Nippon Steel Corporation,Sumitomo (SEI) Steel Wire Corp.
- 当前专利权人地址: JP Kobe-shi JP Tokyo JP Itami-shi
- 优先权: JP2005-348182 20051201
- 国际申请: PCT/JP2006/323963 WO 20061130
- 主分类号: B32B15/02
- IPC分类号: B32B15/02 ; C25D7/06 ; B60C9/00
摘要:
A rubber-cord complex having an improved wet heat adhesive property between a rubber and a cord comprising a drawn plated wire, and including a metal cord comprising a drawn plated wire prepared by providing a brass plated layer on the surface of an element wire and drawing the resulting plated wire, and a rubber vulcanized and bonded to the cord, wherein in a wet heat deterioration state of the drawn plated wire after being subjected to the vulcanization to bond the rubber thereto and further held under an atmosphere having a temperature of 50 to 100° C. and a humidity of 60 to 100% for one hour to 20 days, the average grain size of crystal grains present in the brass plated layer is not more than 50 nm, and the grain boundary of the crystal grains has a fractal dimension of 1.001 to 1.500.