US20100018142A1 METHOD OF MANUFACTURING A FIRE RETARDANT COMPOSITE, A COMPOSITE AND ITS USE
审中-公开
制备阻燃复合材料的方法,复合材料及其用途
- Patent Title: METHOD OF MANUFACTURING A FIRE RETARDANT COMPOSITE, A COMPOSITE AND ITS USE
- Patent Title (中): 制备阻燃复合材料的方法,复合材料及其用途
-
Application No.: US12523831Application Date: 2008-01-23
-
Publication No.: US20100018142A1Publication Date: 2010-01-28
- Inventor: Peter Willem Marie Schouren , Eric Peter Wilhelmus Elisabeth Smeets , Moses Rathbun , Abraham Araya , Henricus Johanna De Swart , Wilhelmus Petrus Theodorus Kemperman , Jan Noordegraaf , Petrus Erederikus Maria Rensen , Christianus Marcus Gijsbertus Maria Buijk
- Applicant: Peter Willem Marie Schouren , Eric Peter Wilhelmus Elisabeth Smeets , Moses Rathbun , Abraham Araya , Henricus Johanna De Swart , Wilhelmus Petrus Theodorus Kemperman , Jan Noordegraaf , Petrus Erederikus Maria Rensen , Christianus Marcus Gijsbertus Maria Buijk
- Priority: GB0701245.3 20070123; NL1033269 20070123
- International Application: PCT/NL08/00025 WO 20080123
- Main IPC: E04C2/20
- IPC: E04C2/20 ; B29C67/20 ; C09D5/18 ; C08J9/22

Abstract:
A method of manufacturing a fire retardant composite, a composite and its use. A method of manufacturing a fire retardant composite by applying an aqueous gel-forming composition, e.g. a fire retardant coating composition, on a substrate comprises an aluminosilicate, the aluminosilicate comprising alkali metal aluminate and an alkali metal silicate, and an organic liquid having a boiling point greater than 110° C., e.g. silicone oil. The molar ratio of SiO2:X2O for the alkali metal silicate is from 3.6:1 to 10:1, where X represents the alkali metal of the alkali metal silicate, when the alkali metal aluminate has a molar ratio of Y2O:AI2O3 of 1.35:1, where Y represents the alkali metal of the alkali metal aluminate, this providing improved water resistance for films or coatings prepared from the compositions by drying and curing.