发明申请
- 专利标题: HIGH CLEANLINESS SPRING STEEL AND HIGH CLEANLINESS SPRING EXCELLENT IN FATIGUE PROPERTIES
- 专利标题(中): 高清洁弹簧钢和高清洁弹性优异的疲劳性能
-
申请号: US12683672申请日: 2010-01-07
-
公开(公告)号: US20100111748A1公开(公告)日: 2010-05-06
- 发明人: Tomoko SUGIMURA , Sei Kimura , Koichi Sakamoto , Atsuhiko Yoshida , Takeshi Inoue
- 申请人: Tomoko SUGIMURA , Sei Kimura , Koichi Sakamoto , Atsuhiko Yoshida , Takeshi Inoue
- 申请人地址: JP Kobe-shi
- 专利权人: Kabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.)
- 当前专利权人: Kabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.)
- 当前专利权人地址: JP Kobe-shi
- 优先权: JP2006-160796 20060609; JP2006-161240 20060609
- 主分类号: C22C38/46
- IPC分类号: C22C38/46 ; C22C38/00 ; C22C38/02 ; C22C38/12
摘要:
High cleanliness spring steel useful in manufacturing a spring with SiO2-based inclusions being extremely controlled and excellent in fatigue properties is provided.High cleanliness spring steel which is steel containing;C: 1.2% (means mass %, hereafter the same with respect to the component) or below (not inclusive of 0%), Si: 1.2-4%, Mn: 0.1-2.0%, Al: 0.01% or below (not inclusive of 0%), and the balance comprising iron with inevitable impurities, wherein; the total of oxide-based inclusions of 4 or above of L (the large diameter of an inclusion)/D (the short diameter of an inclusion) and 25 μm or above of D and oxide-based inclusions of less than 4 L/D and 25 μm or above of L, in the oxide-based inclusions of 25 mass % or above of oxygen concentration and 70% (means mass %, hereafter the same with respect to inclusions) or above of SiO2 content when Al2O3+MgO+CaO+SiO2+MnO=100% is presumed, out of inclusions in the steel, is 20 nos./500 g or below.