US20100243557A1 ALUMINA POROUS BODY AND METHOD OF PRODUCING THE SAME 审中-公开
铝多孔体及其制造方法

ALUMINA POROUS BODY AND METHOD OF PRODUCING THE SAME
Abstract:
An alumina porous body has a porosity of 15 to 45% and an average pore size of 2 to 15 μm includes 5 to 30 mass % of titanium oxide and at least one element selected from the group consisting of copper, manganese, calcium, and strontium, the total content of oxides of the at least one element being 1.5 mass % or less.