发明申请
- 专利标题: ALUMINUM ALLOY FOR CASTING HAVING HIGH RIGIDITY AND LOW LINEAR EXPANSION COEFFICIENT
- 专利标题(中): 具有高刚性和低线性膨胀系数的铝合金
-
申请号: US12848859申请日: 2010-08-02
-
公开(公告)号: US20100296964A1公开(公告)日: 2010-11-25
- 发明人: Kazuhiro ODA , Masahiko Shioda
- 申请人: Kazuhiro ODA , Masahiko Shioda
- 申请人地址: JP Shinagawa-ku
- 专利权人: NIPPON LIGHT METAL COMPANY, LTD.
- 当前专利权人: NIPPON LIGHT METAL COMPANY, LTD.
- 当前专利权人地址: JP Shinagawa-ku
- 优先权: JP2004-084256 20040323
- 主分类号: C22C21/02
- IPC分类号: C22C21/02 ; C22C21/08 ; C22C21/16 ; C22C21/14
摘要:
[Objectives] An aluminum alloy for casting with excellent rigidity and having a low coefficient of linear expansion, and at the same time, does not have a high cost, and has a few restrictions at the time of recycling.[Means for Achieving Objectives] An aluminum alloy for casting with excellent rigidity and having a low coefficient of linear expansion containing 13-25% by mass of silicon, 2-8% by mass of copper, 0.5-3% by mass of iron, 0.3-3% by mass of manganese, 0.001-0.02% by mass of phosphorus, and the remainder comprising aluminum and inevitable impurities, wherein the total amount of iron and manganese is 3.0% by mass or greater. Said alloy may further contain 0.5-6% by mass of nickel, and the total amount of iron, manganese, and nickel may be 3.0% by mass or greater. Further, said alloy may further contain one or more of 0.1-1.0% by mass of chromium, 0.05-1.5% by mass of magnesium, 0.01-1.0% by mass of titanium, 0.0001-1.0% by mass of boron, 0.1-1.0% by mass of zirconium, 0.1-1.0% by mass of vanadium, or 0.01-1.0% by mass of molybdenum.