发明申请
US20120125491A1 Method for the Hot-Dip Coating of a Flat Steel Product Containing 2 - 35 wt.% of Mn, and a Flat Steel Product
有权
含有2-35重量%的Mn和扁钢产品的扁钢产品的热浸涂覆方法
- 专利标题: Method for the Hot-Dip Coating of a Flat Steel Product Containing 2 - 35 wt.% of Mn, and a Flat Steel Product
- 专利标题(中): 含有2-35重量%的Mn和扁钢产品的扁钢产品的热浸涂覆方法
-
申请号: US13265573申请日: 2010-04-22
-
公开(公告)号: US20120125491A1公开(公告)日: 2012-05-24
- 发明人: Manfred Meurer , Martin Norden , Wilhelm Warnecke , Marc Blumenau , Matthias Dahlem , Jennifer Schulz , Klaus Josef Peters
- 申请人: Manfred Meurer , Martin Norden , Wilhelm Warnecke , Marc Blumenau , Matthias Dahlem , Jennifer Schulz , Klaus Josef Peters
- 申请人地址: DE Duisburg
- 专利权人: THYSSENKRUPP STEEL EUROPE AG
- 当前专利权人: THYSSENKRUPP STEEL EUROPE AG
- 当前专利权人地址: DE Duisburg
- 优先权: DE102009018577.1 20090423
- 国际申请: PCT/EP10/55334 WO 20100422
- 主分类号: C23C2/02
- IPC分类号: C23C2/02 ; C21D6/00
摘要:
A method by which a flat steel product containing 2-35 wt. % of Mn can be provided with a coating of Zn which adheres well by annealing at an annealing temperature Ta of 600-1100° C. for an annealing time of 10-240 s under an annealing atmosphere which has a reducing effect on the FeO present on the flat steel product and an oxidising effect on the Mn contained in the steel substrate thereby forming a layer of Mn mixed oxide which covers the flat steel product at least in sections and then cooling the flat steel product to a temperature for bath entry and conveying it through a bath of molten Zn saturated within iron at a temperature of 420-520° C., within a dip time of 0.1-10 s.