发明申请
US20120241055A1 PROCESS FOR PRODUCING BRAKE PISTON 审中-公开
生产制动活塞的方法

  • 专利标题: PROCESS FOR PRODUCING BRAKE PISTON
  • 专利标题(中): 生产制动活塞的方法
  • 申请号: US13501816
    申请日: 2010-10-15
  • 公开(公告)号: US20120241055A1
    公开(公告)日: 2012-09-27
  • 发明人: Yasuo Okamoto
  • 申请人: Yasuo Okamoto
  • 申请人地址: JP Minato-ku, Tokyo
  • 专利权人: SHOWA DENKO K.K.
  • 当前专利权人: SHOWA DENKO K.K.
  • 当前专利权人地址: JP Minato-ku, Tokyo
  • 优先权: JP2009-239295 20091016
  • 国际申请: PCT/JP2010/068124 WO 20101015
  • 主分类号: C22F1/043
  • IPC分类号: C22F1/043 C22F1/047 C22F1/05
PROCESS FOR PRODUCING BRAKE PISTON
摘要:
A brake piston having required mechanical strength is produced through fewer steps than in conventional processes. An aluminum alloy containing Si and Mg, wherein the aluminum alloy has a Si concentration (CSi, mass %) and a Mg concentration (CMg mass %) falling within a range surrounded by four points A (0.75, 1.25), B (1.4, 1), C (1.4, 0.6), and D (0.75, 0.85) in terms of a relationship thereof (CSi, CMg), and further has a Cu concentration of 0.07 to 0.9 mass %, a Mn concentration of 0.1 to 0.9 mass %, a Ti concentration of 0.005 to 0.15 mass %, a Cr concentration of 0.2 mass % or less, and a Fe concentration of 0.5 mass or less %, the balance being A1 and inevitable impurities is cast to obtain a rod-shaped ingot. The rod-shaped ingot, without being subjected to a homogenization treatment, is straightened within 3 (three) days after the casting. The straightened rod-shaped ingot is cut into a given thickness to obtain a forging raw material. This forging raw material, without being subjected to annealing, is cold-forged at a reduction rate of 25 to 90% within 7 (seven) days after the casting of the rod-shaped ingot into a cup shape, which is subjected to age-hardening without being subjected to a solution heat treatment.