发明申请
US20120276454A1 NICKEL COMPLEX HYDROXIDE PARTICLES AND NONAQUEOUS ELECTROLYTE SECONDARY BATTERY 有权
镍系复合氢氧化物颗粒和非水电解质二次电池

  • 专利标题: NICKEL COMPLEX HYDROXIDE PARTICLES AND NONAQUEOUS ELECTROLYTE SECONDARY BATTERY
  • 专利标题(中): 镍系复合氢氧化物颗粒和非水电解质二次电池
  • 申请号: US13513240
    申请日: 2010-12-02
  • 公开(公告)号: US20120276454A1
    公开(公告)日: 2012-11-01
  • 发明人: Kensaku MoriShin ImaizumiRei Kokado
  • 申请人: Kensaku MoriShin ImaizumiRei Kokado
  • 优先权: JP2009-274550 20091202
  • 国际申请: PCT/JP2010/007040 WO 20101202
  • 主分类号: H01M4/525
  • IPC分类号: H01M4/525 C09K3/00
NICKEL COMPLEX HYDROXIDE PARTICLES AND NONAQUEOUS ELECTROLYTE SECONDARY BATTERY
摘要:
Disclosed are: nickel complex hydroxide particles that have small and uniform particle diameters; and a method by which the nickel complex hydroxide particles can be produced. Specifically disclosed is a method for producing a nickel complex hydroxide by a crystallization reaction, which comprises: a nucleation step in which nucleation is carried out, while controlling an aqueous solution for nucleation containing an ammonium ion supplying material and a metal compound that contains nickel to have a pH of 12.0-13.4 at a liquid temperature of 25° C.; and a particle growth step in which nuclei are grown, while controlling an aqueous solution for particle growth containing the nuclei, which have been formed in the nucleation step, to have a pH of 10.5-12.0 at a liquid temperature of 25° C. In this connection, the pH in the particle growth step is controlled to be less than the pH in the nucleation step.