发明申请
- 专利标题: TWO-ELECTRODE WELDING METHOD
- 专利标题(中): 双电极焊接方法
-
申请号: US13471872申请日: 2012-05-15
-
公开(公告)号: US20120312795A1公开(公告)日: 2012-12-13
- 发明人: Reiichi SUZUKI , Kei YAMAZAKI
- 申请人: Reiichi SUZUKI , Kei YAMAZAKI
- 申请人地址: JP Kobe-shi
- 专利权人: Kabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.)
- 当前专利权人: Kabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.)
- 当前专利权人地址: JP Kobe-shi
- 优先权: JP2011-128868 20110609
- 主分类号: B23K9/00
- IPC分类号: B23K9/00
摘要:
In a two-electrode welding method of the present invention, a leading electrode is used to perform gas-shielded arc welding and a trailing electrode is an energized filler. A trailing electrode wire protrudes from a guide lead or guide tip and is energized from an energizing tip. The distance between a welding surface and the energizing tip is 100 mm or more and 1500 mm or less. The distance between electrodes is 10 mm or less. The electric current of the leading electrode is 250 A or more, and the electric current of the trailing electrode is 10 A or more and 50% or less of the electric current of the leading electrode. The feeding speed of the trailing electrode wire is 20% or more and 50% or less of the feeding speed of the leading electrode wire.
公开/授权文献
- US08809740B2 Two-electrode welding method 公开/授权日:2014-08-19