Invention Application
US20150274920A1 EXPANDABLE ACRYLIC RESIN BEAD, EXPANDED ACRYLIC RESIN BEAD, FOAMED MOLDED ARTICLE OF EXPANDED ACRYLIC RESIN BEADS
有权
可膨胀的丙烯酸树脂珠,膨胀的丙烯酸树脂珠,膨胀的丙烯酸树脂珠的泡沫塑料制品
- Patent Title: EXPANDABLE ACRYLIC RESIN BEAD, EXPANDED ACRYLIC RESIN BEAD, FOAMED MOLDED ARTICLE OF EXPANDED ACRYLIC RESIN BEADS
- Patent Title (中): 可膨胀的丙烯酸树脂珠,膨胀的丙烯酸树脂珠,膨胀的丙烯酸树脂珠的泡沫塑料制品
-
Application No.: US14661614Application Date: 2015-03-18
-
Publication No.: US20150274920A1Publication Date: 2015-10-01
- Inventor: Jumpei GOTO , Yota KUWADA
- Applicant: JSP CORPORATION
- Applicant Address: JP Chiyoda-ku
- Assignee: JSP CORPORATION
- Current Assignee: JSP CORPORATION
- Current Assignee Address: JP Chiyoda-ku
- Priority: JP2014-061462 20140325
- Main IPC: C08J9/228
- IPC: C08J9/228 ; C08J9/14

Abstract:
Provided are: expandable acrylic resin bead and expanded acrylic resin bead, both having excellent moldability and capable of providing a foamed molded article that generates less soot during combustion and has a low decomposition gas generation speed; and a foamed molded article obtained through in-mold molding the expanded acrylic resin beads.The expandable acrylic resin bead is composed of an acrylic resin and a physical blowing agent impregnated therein. The acrylic resin contains a methacrylic ester component (A) and an acrylic ester component (B). The content of the component (A) is 85 to 99 mol % with respect to a total 100 mol % of the component (A) and the component (B). At least one of the component (A) and the component (B) contains a component having a polycyclic saturated hydrocarbon group. The glass transition temperature of the acrylic resin is 112 to 125° C.