PROCESS FOR MAKING A LITHIATED OXIDE
Abstract:
Process for making a lithiated oxide, said process comprising the following steps: (a) making a particulate hydroxide, oxide or oxyhydroxide of nickel, and, optionally, at least one of Co and Mn and, by combining an aqueous solution of sodium or potassium hydrox-ide with an aqueous solution containing a water-soluble salt of nickel and, optionally, a water-soluble salt of Co, Mn, Al, Ti, Zr, W, Mo, Ga, Nb, Ta, or Mg, (b) adding a source of lithium, (c) treating the mixture obtained from step (b) thermally at at least two different temperatures: (c1) at 300 to 500° C. under an atmosphere that may comprise oxygen, (c2) at 500 to 600° C. under an atmosphere of oxygen, wherein the temperature in step (c2) is set to be higher than in step (c1).