Manufacturing process for high temperature carburized case harden steel
摘要:
A case hardening steel which consists essentially of 0.03-0.2 wt % of C, 1.0-3.0 wt % of Si, 0.2-2.0 wt % of Mn, 0.05-0.5 wt % of V and the balance of Fe. The primary advantage of this steel is fineness of grain size after carburizing at relatively high temperatures. Even when carburizeed at or above 950.degree. C., the grain size number is not smaller than 6 in both the hardened case and the core. Optionally the steel may contain up to 2.0 wt % of Ni, up to 2.0 wt % of Cr and/or up to 0.5 wt % of Mo for the reinforcing purpose, and/or up to 0.1 wt % of Al, up to 0.3 wt % of Ti, up to 0.1 wt % of Zr, up to 0.03 wt % of N and/or up to 0.5 wt % of Nb+Ta for the purpose of depressing the grain growth.