A large, austenitic, non-magnetic, stainless steel, alloy article which has been significantly warm worked between about 1500 F. and 1650 F. but not subsequently annealed, which has a 0.2% yield strength of at least about 90 ksi, and which, when formed into a U-bend, does not undergo stress corrosion cracking within about 700 hours in boiling saturated aqueous sodium chloride containing 2 weight percent (w/o) ammonium bisulfite. The alloy of the article consists essentially of about:______________________________________ Elements w/o ______________________________________ C 0.1 Max. Mn 1-11 Si 0.6 Max. Cr 18-23 Ni 14-25 Mo 2.5-6.5 Cu 2 Max. B .01 Max. N 0.15 Min. C + N .gtoreq. ##STR1## ______________________________________ and the balance is essentially iron. A preferred alloy for this article contains about:______________________________________ Elements w/o ______________________________________ C .02 Max. Mn 3.0-9.0 Si 0.5 Max. Cr 18-23 Ni 15-22 Mo 2.5-6.5 N 0.20 Min. 3 Mo + Cr .gtoreq. 29.5 ______________________________________
公开/授权文献
信息查询
0/0