发明授权
US5691070A Polyolefin composition, molded article thereof and multilayered laminate
失效
聚烯烃组合物,其成型体和多层层压体
- 专利标题: Polyolefin composition, molded article thereof and multilayered laminate
- 专利标题(中): 聚烯烃组合物,其成型体和多层层压体
-
申请号: US661544申请日: 1996-06-11
-
公开(公告)号: US5691070A公开(公告)日: 1997-11-25
- 发明人: Kazuyuki Watanabe , Satoshi Iwamoto
- 申请人: Kazuyuki Watanabe , Satoshi Iwamoto
- 申请人地址: JPX Tokyo
- 专利权人: Showa Denko K.K.
- 当前专利权人: Showa Denko K.K.
- 当前专利权人地址: JPX Tokyo
- 优先权: JPX5-280240 19931013
- 主分类号: C08J5/18
- IPC分类号: C08J5/18 ; B29C45/00 ; B29C49/00 ; B29K23/00 ; B32B27/32 ; C08L23/00 ; C08L23/02 ; C08L23/04 ; C08L23/06 ; C08L23/10 ; C08L23/12 ; C08L23/14 ; B32B1/02 ; B65D30/08
摘要:
A polyolefin composition, which comprises: (A) 1 to 99% by weight of a polyolefin having the following properties of (a) to (e); (a) a ratio of kinematic viscosity .eta..sub.1 at a frequency of 10.sup.-1 rad/sec to kinematic viscosity .eta..sub.2 at a frequency of 10 rad/sec at a temperature of 190.degree. C. according to a kinematic viscoelasticity determination method of 4 to 20, (b) a crystallization peak temperature Tcp according to a Differential Scanning Calorimetry of 110.degree. C. to 130.degree. C., (c) a ratio (Tmp/Tcp) of melting peak temperature Tmp to crystallization peak temperature Tcp according to a Differential Scanning Calorimetry of 1.1 to 1.5, (d) Tmp/(Tmp-Tcp)=3.0 to 9.8, and (e) a crystal structure exhibiting a-axial orientation in a diffraction pattern according to a X-ray diffraction method, and (B) 99 to 1% by weight of a propylene resin having the following properties of (f) and (g); (f) a ratio of kinematic viscosity .eta..sub.1 at a frequency of 10.sup.-1 rad/sec to kinematic viscosity .eta..sub.2 at a frequency of 10 rad/sec at a temperature of 190.degree. C. according to a kinematic viscoelasticity determination method of below 4, and (e) and no crystallization structure exhibiting a-axial orientation in a diffraction pattern according to a X-ray diffraction method.
公开/授权文献
信息查询