发明授权
- 专利标题: Magnetically biasing bond magnet for improving DC superposition characteristics of magnetic coil
- 专利标题(中): 用于改善电磁线圈直流叠加特性的磁偏置磁铁
-
申请号: US09950568申请日: 2001-09-10
-
公开(公告)号: US06856231B2公开(公告)日: 2005-02-15
- 发明人: Teruhiko Fujiwara , Masayoshi Ishii , Haruki Hoshi , Keita Isogai , Hatsuo Matsumoto , Toru Ito , Tamiko Ambo
- 申请人: Teruhiko Fujiwara , Masayoshi Ishii , Haruki Hoshi , Keita Isogai , Hatsuo Matsumoto , Toru Ito , Tamiko Ambo
- 申请人地址: JP Miyagi
- 专利权人: NEC Tokin Corporaton
- 当前专利权人: NEC Tokin Corporaton
- 当前专利权人地址: JP Miyagi
- 代理机构: Frishauf, Holtz, Goodman & Chick, P.C.
- 优先权: JP2000-272656 20000908; JP2000-325858 20001025; JP2000-352722 20001120; JP2000-356669 20001122; JP2000-356705 20001122; JP2000-360646 20001128; JP2000-360866 20001128; JP2000-361077 20001128; JP2001-022892 20010131; JP2001-117665 20010417
- 主分类号: H01F1/055
- IPC分类号: H01F1/055 ; H01F3/10 ; H01F3/14 ; H01F17/04 ; H01F29/14 ; H01F27/24
摘要:
In order to provide an inductance part having excellent DC superposition characteristic and core-loss, a magnetically biasing magnet, which is disposed in a magnetic gap of a magnetic core, is a bond magnet comprising magnetic powder and plastic resin with the content of the resin being 20% or more on the base of volumetric ratio and which has a specific resistance of 0.1Ω•cm or more. The magnetic powder used is rare-earth magnetic powder having an intrinsic coercive force of 5 kOe or more, Curie point of 300° C. or more, and an average particle size of 2.0-50 μm. A magnetically biasing magnet used in an inductance part that is treated by the reflow soldering method has a resin content of 30% or more and the magnetic powder used therein is Sm—Co magnetic powder having an intrinsic coercive force of 10 kOe or more, Curie point of 500° C. or more, and an average particle size of 2.5-50 μm. A thin magnet having a thickness of 500 μm or less can be realized for a small-sized inductance part.
公开/授权文献
信息查询