- 专利标题: High strength steel weld having improved resistance to cold cracking and a welding method
-
申请号: US10334717申请日: 2003-01-02
-
公开(公告)号: US06953508B2公开(公告)日: 2005-10-11
- 发明人: Tomoaki Ikeda , Akio Yamamoto , Shigemichi Yamauchi , Nobuaki Takahashi , Masahiko Hamada
- 申请人: Tomoaki Ikeda , Akio Yamamoto , Shigemichi Yamauchi , Nobuaki Takahashi , Masahiko Hamada
- 申请人地址: JP Osaka
- 专利权人: Sumitomo Metal Industries, Ltd.
- 当前专利权人: Sumitomo Metal Industries, Ltd.
- 当前专利权人地址: JP Osaka
- 代理机构: Clark & Brody
- 主分类号: B23K9/18
- IPC分类号: B23K9/18 ; C21D1/84 ; C21D9/50 ; C22C38/42 ; C22C38/44 ; C22C38/46 ; C22C38/48 ; C22C38/54 ; C22C38/58 ; C22C38/02 ; C22C38/06 ; C22C38/14
摘要:
A welding method includes performing welding to form a weld metal consisting essentially of, in mass %, C: 0.01-0.15%,Si: 0.02-0.6%,Mn: 0.6-3.0%, Al: 0.004-0.08%,Ti: 0.003-0.03%,B: at most 0.005%, Cu: 0-1.2%,Ni: 0-3%,Cr: 0-1.2%, Mo: 0-2%,V: 0-0.05%,Nb: 0-0.05%, and a remainder of Fe and unavoidable impurities. The amounts of impurities are P: at most 0.03%, S: at most 0.03%, N: at most 0.01%, Ca or Mg: at most 0.005%. The value of Pcm expressed by the following Equation (3) is in the range of 0.23-0.35%, and the time T until the weld metal is cooled to 100° C. after welding satisfies the following Equation (1): T(seconds)≧exp(7.0×Pw+4.66) Equation (1) Pw=Pcm+HD/60 Equation (2) Pcm(mass %)=C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B Equation (3) HD [ml/100 g]: amount of hydrogen in the weld metal immediately after welding.