- 专利标题: Nickel electrode material, and production method therefor, and nickel electrode and alkaline battery
- 专利标题(中): 镍电极材料及其制造方法,镍电极和碱性电池
-
申请号: US10486906申请日: 2002-09-03
-
公开(公告)号: US07635512B2公开(公告)日: 2009-12-22
- 发明人: Seijiro Ochiai , Mitsuhiro Kodama , Kengo Furukawa , Toshiki Tanaka , Minoru Kuzuhara , Masaharu Watada , Masahiko Oshitani
- 申请人: Seijiro Ochiai , Mitsuhiro Kodama , Kengo Furukawa , Toshiki Tanaka , Minoru Kuzuhara , Masaharu Watada , Masahiko Oshitani
- 申请人地址: JP Takatsuki-shi, Osaka
- 专利权人: Yuasa Corporation
- 当前专利权人: Yuasa Corporation
- 当前专利权人地址: JP Takatsuki-shi, Osaka
- 代理机构: McGinn IP Law Group, PLLC
- 优先权: JP2001-265607 20010903; JP2001-267354 20010904; JP2001-311218 20011009; JP2001-348245 20011114
- 国际申请: PCT/JP02/08919 WO 20020903
- 国际公布: WO03/021698 WO 20030313
- 主分类号: B32B3/04
- IPC分类号: B32B3/04 ; H01M4/00
摘要:
For accomplishing the subjects, the invention provides a nickel electrode material for use in a nickel electrode, wherein the positive-electrode material constituting the electrode material comprises: positive active material particles which comprise as the main component either a nickel hydroxide or a solid solution in a nickel hydroxide of one or more other elements and in which part of the nickel hydroxide has been oxidized; and a coating layer formed on the surface of the positive active material particles and comprising as the main component a high-order cobalt compound in which the cobalt has an oxidation number larger than 2, the average oxidation number of the nickel in the positive active material particles and the cobalt in the coating layer being from 2.04 to 2.40, and the positive-electrode material having a tap density of 2.0 g/cm3 or higher. The invention further provides a process for producing the electrode material, a nickel electrode employing the electrode material, and an alkaline storage battery having the nickel electrode.