发明授权
- 专利标题: Electrode plate of positive electrode for non-aqueous electrolyte secondary battery and manufacturing method thereof
- 专利标题(中): 非水电解质二次电池用正极用电极板及其制造方法
-
申请号: US11146350申请日: 2005-06-07
-
公开(公告)号: US07662516B2公开(公告)日: 2010-02-16
- 发明人: Masao Fukunaga , Kohei Suzuki , Katsumi Kashiwagi , Akira Kuroda , Yasuhiro Inadomi , Masanori Sumihara
- 申请人: Masao Fukunaga , Kohei Suzuki , Katsumi Kashiwagi , Akira Kuroda , Yasuhiro Inadomi , Masanori Sumihara
- 申请人地址: JP Osaka
- 专利权人: Panasonic Corporation
- 当前专利权人: Panasonic Corporation
- 当前专利权人地址: JP Osaka
- 代理机构: McDermott Will & Emery LLP
- 优先权: JP2004-168121 20040607; JP2004-168122 20040607; JP2004-168123 20040607; JP2004-168240 20040607; JP2004-168241 20040607; JP2004-168242 20040607
- 主分类号: H01M4/62
- IPC分类号: H01M4/62 ; H01M4/00
摘要:
A method for manufacturing a positive electrode plate for a non-aqueous secondary battery including: preparing an active material A, a conductive material B, a binder C, a thickener D, and a liquid component E, the thickener D being in a powder state, the conductive material B including a carbon material, the thickener D including a water-soluble polymer, and the liquid component E including water; preparing a slurry including the component E and an electrode material mixture, the material mixture including the active material A, the conductive material B, the binder C, and the thickener D; and applying the slurry on a current collector. In preparing the slurry, the thickener D in a powder state, the active material A and the conductive material B are kneaded together with the liquid component E, and then the primary kneaded matter, the binder C, and an additional liquid component are kneaded.