发明授权
US08137803B2 Multilayer structure polymer and resin composition together with acrylic resin film material, acrylic resin laminate film, photocurable acrylic resin film or sheet, laminate film or sheet and laminate molding obtained by laminating thereof
有权
多层结构聚合物和树脂组合物与丙烯酸树脂膜材料,丙烯酸树脂层压膜,光固化丙烯酸树脂膜或片材,层压膜或片材以及通过层压获得的层压成型
- 专利标题: Multilayer structure polymer and resin composition together with acrylic resin film material, acrylic resin laminate film, photocurable acrylic resin film or sheet, laminate film or sheet and laminate molding obtained by laminating thereof
- 专利标题(中): 多层结构聚合物和树脂组合物与丙烯酸树脂膜材料,丙烯酸树脂层压膜,光固化丙烯酸树脂膜或片材,层压膜或片材以及通过层压获得的层压成型
-
申请号: US12831436申请日: 2010-07-07
-
公开(公告)号: US08137803B2公开(公告)日: 2012-03-20
- 发明人: Yukio Kitaike , Yoshinori Abe , Junichi Abe , Koichiro Kitashima , Shogo Okazaki , Hideyuki Fujii
- 申请人: Yukio Kitaike , Yoshinori Abe , Junichi Abe , Koichiro Kitashima , Shogo Okazaki , Hideyuki Fujii
- 申请人地址: JP Tokyo
- 专利权人: Mitsubishi Rayon Co., Ltd.
- 当前专利权人: Mitsubishi Rayon Co., Ltd.
- 当前专利权人地址: JP Tokyo
- 代理机构: Oblon, Spivak, McClelland, Maier & Neustadt, L.L.P.
- 优先权: JP2003-004427 20030110; JP2003-041212 20030219; JP2003-057335 20030304; JP2003-058554 20030305; JP2003-058690 20030305; JP2003-058692 20030305; JP2003-066645 20030312; JP2003-069915 20030314
- 主分类号: B32B27/30
- IPC分类号: B32B27/30
摘要:
An acrylic resin film material comprising at least a multilayer structure polymer with a particular structure prevent a molded item from being whitened during insert- or in-mold molding and meet the requirement for surface hardness, heat resistance, and transparency or matting performance for vehicle applications. It is also possible to use an acrylic resin film material exhibiting a difference of 30% or less between haze values as determined in accordance with the testing method of JIS K7136 (haze measurement method) after and before a tensile test where a test piece with a width of 20 mm is pulled under the conditions of an initial inter-chuck distance of 25 mm, a rate of 50 mm/min and a temperature of 23° C. until an end-point inter-chuck distance becomes 33 mm as well as having a pencil hardness of 2 B or higher as determined in accordance with JIS K5400.