发明授权
US08431857B2 Process for joining brass part and silicone carbide ceramics part and composite articles made by same
有权
用于连接黄铜部件和碳化硅陶瓷部件的方法以及由其制成的复合制品
- 专利标题: Process for joining brass part and silicone carbide ceramics part and composite articles made by same
- 专利标题(中): 用于连接黄铜部件和碳化硅陶瓷部件的方法以及由其制成的复合制品
-
申请号: US13166333申请日: 2011-06-22
-
公开(公告)号: US08431857B2公开(公告)日: 2013-04-30
- 发明人: Hsin-Pei Chang , Wen-Rong Chen , Huann-Wu Chiang , Cheng-Shi Chen , Wen-Feng Hu
- 申请人: Hsin-Pei Chang , Wen-Rong Chen , Huann-Wu Chiang , Cheng-Shi Chen , Wen-Feng Hu
- 申请人地址: CN Shenzhen TW New Taipei
- 专利权人: Hong Fu Jin Precision Industry (ShenZhen) Co., Ltd.,Hon Hai Precision Industry Co., Ltd.
- 当前专利权人: Hong Fu Jin Precision Industry (ShenZhen) Co., Ltd.,Hon Hai Precision Industry Co., Ltd.
- 当前专利权人地址: CN Shenzhen TW New Taipei
- 代理机构: Altis Law Group, Inc.
- 优先权: CN201010570278 20101202
- 主分类号: B23K11/00
- IPC分类号: B23K11/00
摘要:
A process for joining a brass part and a silicone carbide ceramics part, comprising steps of: providing a metal part made of brass, a ceramic part made of silicone carbide ceramics, a titanium foil and a nickel foil; bring the metal part, ceramic part, titanium foil and nickel foil into contact, with the titanium and nickel foil inserted between the metal part and ceramic part; applying a pressure of about 20 MPa˜60 MPa to the parts to be joined; and simultaneously applying a pulse electric current to the parts while the pressure is applied for heating up the parts to a temperature of about 950° C. to about 1150° C. at a rate of about 50° C./min˜300° C./min, maintaining the temperature for about 20 minutes˜40 minutes.