US08580445B2 Shutdown strategy to avoid carbon corrosion due to slow hydrogen/air intrusion rates
有权
关闭策略,以避免由于氢/空气入侵速率慢而导致的碳腐蚀
- 专利标题: Shutdown strategy to avoid carbon corrosion due to slow hydrogen/air intrusion rates
- 专利标题(中): 关闭策略,以避免由于氢/空气入侵速率慢而导致的碳腐蚀
-
申请号: US12327957申请日: 2008-12-04
-
公开(公告)号: US08580445B2公开(公告)日: 2013-11-12
- 发明人: Thomas A. Greszler , Gary M. Robb , John P. Salvador , Balasubramanian Lakshmanan , Hubert Gasteiger
- 申请人: Thomas A. Greszler , Gary M. Robb , John P. Salvador , Balasubramanian Lakshmanan , Hubert Gasteiger
- 申请人地址: US MI Detroit
- 专利权人: GM Global Technology Operations LLC
- 当前专利权人: GM Global Technology Operations LLC
- 当前专利权人地址: US MI Detroit
- 代理机构: Fraser Clemens Martin & Miller LLC
- 代理商 J. Douglas Miller
- 主分类号: H01M8/06
- IPC分类号: H01M8/06 ; H01M8/04
摘要:
A fuel cell system including a fuel cell stack having a plurality of fuel cells, each of the fuel cells including an electrolyte membrane disposed between an anode and a cathode, an anode supply manifold in fluid communication with the anodes of the fuel cells, the anode supply manifold providing fluid communication between a source of hydrogen and the anodes, an anode exhaust manifold in fluid communication with the anodes of the fuel cells, and a fan in fluid communication with the anodes of the fuel cells, wherein the fan controls a flow of fluid through the anodes of the fuel cells after the fuel cell system is shutdown.