发明授权
US08672020B2 Method for producing aluminum-zirconium-carbon intermediate alloy
有权
铝 - 锆 - 碳中间体合金的生产方法
- 专利标题: Method for producing aluminum-zirconium-carbon intermediate alloy
- 专利标题(中): 铝 - 锆 - 碳中间体合金的生产方法
-
申请号: US13141496申请日: 2011-04-23
-
公开(公告)号: US08672020B2公开(公告)日: 2014-03-18
- 发明人: Xuemin Chen , Qingdong Ye , Yueming Yu , Jianguo Li
- 申请人: Xuemin Chen , Qingdong Ye , Yueming Yu , Jianguo Li
- 申请人地址: CN Shenzhen, Guangdong
- 专利权人: Shenzhen Sunxing Light Alloys Materials Co., Ltd.
- 当前专利权人: Shenzhen Sunxing Light Alloys Materials Co., Ltd.
- 当前专利权人地址: CN Shenzhen, Guangdong
- 代理机构: Jackson IPG PLLC
- 优先权: CN201110060734 20110315
- 国际申请: PCT/CN2011/073217 WO 20110423
- 国际公布: WO2012/027992 WO 20120308
- 主分类号: B22D11/00
- IPC分类号: B22D11/00 ; B22D27/02 ; B22D11/10 ; C22C21/00
摘要:
The present invention discloses a method for producing an aluminum-zirconium-carbon (Al—Zr—C) intermediate alloy; the Al—Zr—C intermediate alloy has a chemical composition of 0.01% to 10% Zr, 0.01% to 0.3% C, and Al in balance; the producing method comprising the steps of: producing commercially pure aluminum, zirconium metal, and graphite material according to the weight percentages of the aluminum-zirconium-carbon intermediate alloy; the graphite is graphite powder having an average particle size of 0.074 mm to 1 mm; and the graphite powder is subjected to the following treatments: being added to the aqueous solution of KF, NaF, K2ZrF6, K2TiF6 or the combination thereof, soaked for 12 to 72 hours, filtrated or centrifuged, and dried at 80° C. to 200° C. for 12 to 24 hours; melting the commercially pure aluminum and keeping it at 700° C. to 900° C. to provide aluminum liquid, in which the prepared zirconium and the treated graphite powder are added and melted to provide an alloy solution; and keeping the alloys solution at 700° C. to 900° C. under mechanical or electromagnetic agitation and performing casting molding. The present method produces a high-quality Al—Zr—C intermediate alloy in low cost.