发明授权
- 专利标题: Transparent zirconia sintered body, method for producing same, and use of same
- 专利标题(中): 透明氧化锆烧结体及其制造方法及其应用
-
申请号: US13380190申请日: 2010-07-15
-
公开(公告)号: US08815760B2公开(公告)日: 2014-08-26
- 发明人: Masahiro Watanabe , Satoshi Kondoh , Koji Tsukuma
- 申请人: Masahiro Watanabe , Satoshi Kondoh , Koji Tsukuma
- 申请人地址: JP Yamaguchi
- 专利权人: Tosoh Corporation
- 当前专利权人: Tosoh Corporation
- 当前专利权人地址: JP Yamaguchi
- 代理机构: Greenblum & Bernstein, P.L.C.
- 优先权: JP2009-184139 20090807
- 国际申请: PCT/JP2010/062005 WO 20100715
- 国际公布: WO2011/016325 WO 20110210
- 主分类号: C04B35/486
- IPC分类号: C04B35/486
摘要:
The subject of the present invention relates to obtaining a zirconia sintered body having excellent in both properties of a translucency and a mechanical strength. The present invention relates to obtaining a high-strength zirconia sintered body having a translucency of an in-line transmission of 50% or more at a sample thickness of 1 mm for visible light at a wavelength of 600 nm and an average flexural strength of 300 MPa or more by subjecting a zirconia primary sintered body having an average grain size of 1 μm or less and a relative density of 92% or more and the crystal phase composed of cubic crystals only to HIP treatment at a temperature of 1,250° C. to 1,600° C. and a pressure of at least 50 MPa. The primary sintered body is obtained by maintaining a molded body of a zirconia powder containing 7 mol % to 30 mol % of yttria at 1,100° C. to 1,300° C. for at least 5 hrs or by heating the molded body at a high rate of temperature rise of 500° C./hr or more.