- 专利标题: Low alloy steel for geothermal power generation turbine rotor, and low alloy material for geothermal power generation turbine rotor and method for manufacturing the same
- 专利标题(中): 地热发电用转子用低合金钢,地热发电用转子用低合金材料及其制造方法
-
申请号: US13448770申请日: 2012-04-17
-
公开(公告)号: US09034121B2公开(公告)日: 2015-05-19
- 发明人: Satoru Ohsaki , Kazuhiro Miki , Tsukasa Azuma , Koji Kajikawa , Shigeru Suzuki , Masayuki Yamada , Itaru Murakami , Kenichi Okuno , Liang Yan , Reki Takaku , Akihiro Taniguchi , Tetsuya Yamanaka , Makoto Takahashi , Kenichi Imai , Osamu Watanabe , Joji Kaneko
- 申请人: Satoru Ohsaki , Kazuhiro Miki , Tsukasa Azuma , Koji Kajikawa , Shigeru Suzuki , Masayuki Yamada , Itaru Murakami , Kenichi Okuno , Liang Yan , Reki Takaku , Akihiro Taniguchi , Tetsuya Yamanaka , Makoto Takahashi , Kenichi Imai , Osamu Watanabe , Joji Kaneko
- 申请人地址: JP Tokyo JP Tokyo
- 专利权人: THE JAPAN STEEL WORKS,LTD.,KABUSHIKI KAISHA TOSHIBA
- 当前专利权人: THE JAPAN STEEL WORKS,LTD.,KABUSHIKI KAISHA TOSHIBA
- 当前专利权人地址: JP Tokyo JP Tokyo
- 代理机构: Sughrue Mion, PLLC
- 优先权: JP2011-092340 20110418
- 主分类号: C22C38/46
- IPC分类号: C22C38/46 ; C21D6/00 ; C22C38/58 ; C22C38/44 ; C21D7/13 ; C21D1/25 ; C21D1/28
摘要:
A low alloy steel ingot contains from 0.15 to 0.30% of C, from 0.03 to 0.2% of Si, from 0.5 to 2.0% of Mn, from 0.1 to 1.3% of Ni, from 1.5 to 3.5% of Cr, from 0.1 to 1.0% of Mo, and more than 0.15 to 0.35% of V, and optionally Ni, with a balance being Fe and unavoidable impurities. Performing quality heat treatment including a quenching step and a tempering step to the low alloy steel ingot to obtain a material, which has a grain size number of from 3 to 7 and is free from pro-eutectoid ferrite in a metallographic structure thereof, and which has a tensile strength of from 760 to 860 MPa and a fracture appearance transition temperature of not higher than 40° C.