Invention Grant
US09434830B2 Expandable acrylic resin bead, expanded acrylic resin bead, foamed molded article of expanded acrylic resin beads
有权
可膨胀丙烯酸树脂珠,膨胀丙烯酸树脂珠,膨胀丙烯酸树脂珠的发泡模塑制品
- Patent Title: Expandable acrylic resin bead, expanded acrylic resin bead, foamed molded article of expanded acrylic resin beads
- Patent Title (中): 可膨胀丙烯酸树脂珠,膨胀丙烯酸树脂珠,膨胀丙烯酸树脂珠的发泡模塑制品
-
Application No.: US14661614Application Date: 2015-03-18
-
Publication No.: US09434830B2Publication Date: 2016-09-06
- Inventor: Jumpei Goto , Yota Kuwada
- Applicant: JSP CORPORATION
- Applicant Address: JP Chiyoda-ku
- Assignee: JSP CORPORATION
- Current Assignee: JSP CORPORATION
- Current Assignee Address: JP Chiyoda-ku
- Agency: Oblon, McClelland, Maier & Neustadt, L.L.P.
- Priority: JP2014-061462 20140325
- Main IPC: C08J9/14
- IPC: C08J9/14 ; C08J9/228 ; C08J9/18 ; C08J9/224 ; C08J9/232

Abstract:
Provided are: expandable acrylic resin bead and expanded acrylic resin bead, both having excellent moldability and capable of providing a foamed molded article that generates less soot during combustion and has a low decomposition gas generation speed; and a foamed molded article obtained through in-mold molding the expanded acrylic resin beads. The expandable acrylic resin bead is composed of an acrylic resin and a physical blowing agent impregnated therein. The acrylic resin contains a methacrylic ester component (A) and an acrylic ester component (B). The content of the component (A) is 85 to 99 mol % with respect to a total 100 mol % of the component (A) and the component (B). At least one of the component (A) and the component (B) contains a component having a polycyclic saturated hydrocarbon group. The glass transition temperature of the acrylic resin is 112 to 125° C.