- Patent Title: Swellable pre-treatment coating
- Patent Title (中): 可膨胀的预处理涂层
-
Application No.: US14654963Application Date: 2013-01-31
-
Publication No.: US09505938B2Publication Date: 2016-11-29
- Inventor: Bor-Jiunn Niu , Haigang Chen , Jason Swei , Sandeep Bangaru
- Applicant: HEWLETT-PACKARD DEVELOPMENT COMPANY, L.P.
- Applicant Address: US TX Houston
- Assignee: Hewlett-Packard Development Company, L.P.
- Current Assignee: Hewlett-Packard Development Company, L.P.
- Current Assignee Address: US TX Houston
- Agency: Thorpe, North & Western L.L.P.
- International Application: PCT/US2013/024064 WO 20130131
- International Announcement: WO2014/120186 WO 20140807
- Main IPC: B41M5/00
- IPC: B41M5/00 ; C09D7/12 ; B41M5/52 ; C09D129/04 ; C09D177/00 ; C09D179/02 ; C08G73/02 ; C08L91/06

Abstract:
The present disclosure provides swellable pre-treatment compositions, printable media, and related methods. As such, a swellable pre-treatment coating for a print medium can include an evaporable solvent, a matrix, and a wax. The matrix can include from 10 wt % to 20 wt % of a fixer, from 25 wt % to 35 wt % of aluminum chlorohydrate, from 0.5 wt % to 10 wt % of a first binder, from 20 wt % to 30 wt % of a second cross-linkable binder, and from 1 wt % to 5 wt % of a cross-linker. The wax can be present at from 10 wt % to 20 wt %, The weight percentages of the matrix and the wax are based on a total amount present in the swellable pre-treatment coating after removal of the evaporable solvent.