WO2005106377A3 GUN BARREL AND METHOD OF FORMING 审中-公开
枪条和形成方法

GUN BARREL AND METHOD OF FORMING
摘要:
A fabrication technique is described for producing lighter weight and improved wear and erosion resistant gun barrels (10). The barrels (10) are produced in an unconventional manner from the inside bore to the outside diameter of the barrel (10) and combine a refractory metal, metal alloy, or ceramic composite inner liner (12) with a metal matrix composite (MMC) or titanium or other suitable high strength, lightweight metal or metal alloy outer shell. A unique aspect of the invention is that there is a compositional gradation from the liner (12) at the inside bore to the overwrap which extends to the outside diameter of the barrel (10). A process is also described to produce barrels (10) with a refractory metal liner with improved wear and erosion resistance by depositing the refractory metal on the ID of a pre-fabricated barrel (10).