公开(公告)号:EP0815268B1
公开(公告)日:2000-11-22
申请号:EP96927908.2
申请日:1996-08-26
-
2.
公开(公告)号:EP0815268A1
公开(公告)日:1998-01-07
申请号:EP96927908.0
申请日:1996-08-26
发明人: SAKURAI, Koichi , SHIBUYA, Tatsuru , WAKABAYASHI, Hisamoto , WAKI, Kouichi , SUGIYAMA, Seiji , NAGAI, Kazunori
摘要: In a method of continuously annealing steel strip comprising a heating step (A), a soaking step (B), a primary cooling step (C) including a rapid cooling step at least in a second half thereof, an overaging step (D), and a final cooling step (E), inert atmosphere gas containing H2 gas in the concentration of 30 - 60 % is employed as cooling gas for use in the rapid cooling step, the blowoff temperature of the cooling gas is 30 - 150 °C, and the blowoff speed of the cooling gas is 100 - 150 m/sec. The primary cooling method in continuously annealing steel strip provides the primary cooling step (C) including the rapid cooling step which can be carried out with a high efficiency and a low cost.
-