摘要:
Black non-magnetic composite particles for a Black toner of the present invention comprising: (a) hematite and/or iron oxide hydroxide particles having an average particle diameter of from 0.055 to 0.95 µm; (b) a coating on the surface of said hematite and/or iron oxide hydroxide particles, comprising at least one organosilicon compound selected from:(1) organosilane compounds obtainable by drying or heat-treating alkoxysilane compounds,(2) polysiloxanes or modified polysiloxanes, and(3) fluoroalkyl organosilane compounds obtainable by drying or heat-treating fluoroalkylsilane compounds; and (c) carbon black fine particles adhered on said coating, which have a particle diameter of from 0.002 to 0.05 µm and which are present in an amount of from 1 to 25 parts by weight per 100 parts by weight of said hematite and/or iron oxide hydroxide particles.
摘要:
Magnetic particles which have an average particle size of from 10 to 200 µm and which comprise:
magnetic core particles; and a coating layer on the surface of said magnetic core particles, which coat comprises at least one silane-based coupling agent,a silicone resin and at least one metal alkoxide represented by the general formula (I) :
(RO) n M (I)
wherein R is a C 1 to C 16 alkyl group; M is Al, Ti, Na, K, Ca, Zn or Fe; and n is an integer of from 1 to 4.
摘要:
Black magnetic composite particles for a black magnetic toner comprising: (a) magnetic iron oxide particles having an average particle diameter of from 0.055 to 0.95 µm; (b) a coating on the surface of said magnetic iron oxide particles, comprising at least one organosilicon compound selected from: (1) organosilane compounds obtainable by drying or heat-treating alkoxysilane compounds, (2) polysiloxanes or modified polysiloxanes, and (3) fluoroalkyl organosilane compounds obtainable by drying or heat-treating fluoroalkylsilane compounds; and (c) carbon black fine particles adhered on at least a part of said coating, which have a particle size of from 0.002 to 0.05 µm and which are present in an amount of from 1 to 25 parts by weight per 100 parts by weight of said magnetic iron oxide particles.
摘要:
A magnetic recording medium suitably applicable to existent magnetic recording systems using a ring-type magnetic head and capable of using a plastic substrate for providing a magnetic recording medium for high-density recording, which magnetic recording medium has a coercive force of not less than 159 kA/m (2,000 Oe) and comprises: (a) a plastic substrate; and (b) a cobalt-containing maghemite film on the substrate; wherein the film has: a molar ratio of cobalt to iron of not more than 0.06:1; and a spacing of a plane (311) of not more than 0.2510 nm (2.510Å), a spacing of a plane (222) of not more than 0.2415 nm (2.415Å) or a spacing of a plane (220) of not more than 0.2950 nm (2.950Å).
摘要翻译:一种磁记录介质,适用于使用环形磁头的现有磁记录系统,并且能够使用塑料基片来提供用于高密度记录的磁记录介质,该磁记录介质具有不小于159的矫顽力 kA / m(2000 Oe)并且包括:(a)塑料基材; 和(b)在基底上的含钴磁赤铁矿膜; 其中所述膜具有:钴与铁的摩尔比不大于0.06:1; 并且平面(311)的间距不大于0.2510nm(2.510),平面(222)的间距不大于0.2415nm(2.415),或者平面(220)的间隔不大于 超过0.2950nm(2.950)。
摘要:
A pigment for use in paints comprises: a pigment particle as the core particle; a lower coat on at least part of the surface of said pigment particle, comprising squaric acid and/or a polyol having an anthraquinone skeleton represented by the general formula (I): wherein m is 0 or an integer of 1 to 4, n is 0 or an integer of 1 to 4 and m+n is an integer of 2 to 4; and an upper coat on at least part of the surface of said coated particle, comprising at least one alkylene glycol represented by the general formula (II): C q H 2q (OH) 2 (II) wherein q is an integer of 2 to 10.
摘要:
Calcium-iron oxide composite particles of the present invention have a BET specific surface area of 0.1 to 100 m 2 /g and contain iron atoms in an amount of 1 to 500 moles based on 100 moles of calcium atoms, not less than 50 % of iron atoms, based on the total amount of iron atom contained in said calcium-iron oxide composite particles, are bonded with one or more calcium atoms to form a calcium-iron ferrite phase. A hydrogen chloride-scavenger comprising the calcium-iron oxide composite particles, is capable of effectively capturing harmful hydrogen chloride generated by thermal decomposition or combustion of chorine-containing resin molded products upon fire or incineration thereof, and fixing the hydrogen chloride as stable calcium chloride or the like.
a substrate; a nickel oxide underlayer on said substrate; and a cobalt-containing maghemite film which is provided on said nickel oxide underlayer, which has a spacing of a (311) plane of not more than 0.2510 nm (2.510Å), a spacing of a (222) plane of not more than 0.2415 nm (2.415Å) or a spacing of a (220) plane of not more than 0.2950 nm (2.950Å), and in which the ratio of the X-ray diffraction spectrum peak intensity of the (311), (222) or (220) plane of the said film to the X-ray diffraction spectrum peak intensity of the (400) plane is more than 0.5:1.
摘要:
A process for producing lithium-cobalt oxide for use as a cathode active substance for lithium ion batteries, comprises: (a) mixing cobalt oxide having a BET specific surface area of 30 to 200 m 2 /g or an average particle size of not more than 0.1 µm, with a lithium compound; and (b) calcining the obtained mixture at a temperature of 500 to 850°C.