摘要:
A black colorant suitable for ink-jet printing ink, having an average particle diameter of 0.001 to 0.15 µm, and comprising:
an extender pigment as a core particle; a gluing agent-coating layer formed on at least a part of the surface of the core particle; and a black pigment coat formed on at least a part of the gluing agent-coating layer.
The black colorant for ink-jet printing ink exhibits not only a high blackness and an excellent tinting strength, but also excellent dispersibility and light resistance in spite of fine particles.
a non-magnetic base film; and a magnetic recording layer comprising a binder resin and magnetic composite particles which have an average particle diameter of from 0.02 to 0.70 µm and which comprise:
(a) magnetic core particles, (b) a coating provided on the surface of said magnetic core particles, comprising at least one organosilicon compound selected from:
(1) organosilane compounds obtainable from alkoxysilane compounds, and (2) polysiloxanes or modified polysiloxanes, and
(c) a phthalocyanine-based pigment coat which is provided on said coating (b) in an amount of 1 to 100 parts by weight per 100 parts by weight of said magnetic core particles (a).
(i) a non-magnetic base film; (ii) a non-magnetic undercoat layer on the non-magnetic base film, comprising a binder resin and non-magnetic acicular composite particles having an average major axis diameter of 0.01 to 0.3 µm and comprising:
acicular hematite particles or acicular iron oxide hydroxide particles as non-magnetic core particles, a coating on said acicular hematite particles or acicular iron oxide hydroxide particles, comprising at least one organosilicon compound selected from:
(1) organosilane compounds obtainable from alkoxysilane compounds, and (2) polysiloxanes or modified polysiloxanes, and
a phthalocyanine-based pigment coat which is provided on said coating layer and which is present in an amount of from 1 to 100 parts by weight based on 100 parts by weight of said acicular hematite particles or acicular iron oxide hydroxide particles; and
(iii) a magnetic recording layer on the non-magnetic undercoat layer, comprising magnetic particles and a binder resin.
摘要:
Composite particles which have an average particle diameter of from 0.001 to 10.0 µm, comprising:
(i) white inorganic particles as core particles; (ii) a gluing agent coating layer provided on the surface of said white inorganic particles; and (iii) an organic pigment coat provided on said gluing agent coating layer in an amount of from 1 to 500 parts by weight based on 100 parts by weight of said white inorganic particles.
The composite particles may be used in a paint or a rubber or resin composition.
摘要:
A magnetic recording medium comprises a non-magnetic base film; and a magnetic recording layer comprising a binder resin and black magnetic acicular composite particles having an average particle diameter of 0.051 to 0.35 µm and comprising:
magnetic acicular cobalt-coated iron oxide particles or magnetic acicular metal particles containing iron as a main component, a coating on the surface of the magnetic acicular particles, comprising at least one organosilicon compound selected from:
(1) organosilane compounds obtainable from alkoxysilane compounds, and (2) polysiloxanes or modified polysiloxanes, and
a carbon black coat which is provided on the said coating in an amount of from more than 10 to 40 parts by weight per 100 parts by weight of said magnetic acicular particles.
摘要:
Non-magnetic composite particles suitable for use in a magnetic recording medium comprising:
(a) non-magnetic core particles having an average particle size of 0.01 to 0.3 µm; and (b) from 0.1 to 20 % by weight, based on the weight of said non-magnetic core particles, of inorganic particles which have an average particle size of 0.001 to 0.07 µm, which are fixed or anchored on the surface of each non-magnetic core particle through a silicon compound derivable from a tetraalkoxysilane and which comprise at least one inorganic compound selected from oxides, nitrides, carbides and sulfides containing aluminum, zirconium, cerium, titanium, silicon, boron or molybdenum.
a base film; a non-magnetic undercoat layer on said base film, said undercoat layer comprising a binder resin and non-magnetic acicular particles containing iron as a main component and from 0.05 to 50 % by weight of titanium, calculated as Ti, based on the total weight of the particles, which titanium is present within the particles; and a magnetic recording layer on said non-magnetic undercoat layer, said magnetic recording layer comprising magnetic particles and a binder resin.
摘要:
The present invention relates to a process for producing a composite cathode active material for a nonaqueous electrolyte secondary cell which is subjected to surface treatment, comprising: previously mixing the cathode active material with a surface-treating component in the form of a metal compound containing one or more metal elements selected from the group consisting of the first transition series elements and the second transition series elements; and then coating the cathode active material with the surface-treating component using an apparatus capable of effecting a high-speed shearing action.