HIGH MN STEEL SHEET FOR HIGH CORROSION RESISTANCE AND METHOD OF MANUFACTURING GALVANIZING THE STEEL SHEET
    26.
    发明公开
    HIGH MN STEEL SHEET FOR HIGH CORROSION RESISTANCE AND METHOD OF MANUFACTURING GALVANIZING THE STEEL SHEET 有权
    MN-RICH钢用于生产镀锌钢板高耐腐蚀性和方法SHEET

    公开(公告)号:EP1971701A1

    公开(公告)日:2008-09-24

    申请号:EP06835302.8

    申请日:2006-12-20

    申请人: Posco Co., Ltd.

    IPC分类号: C23C2/06

    摘要: A high-manganese hot-dip coated steel sheet is disclosed which provides high corrosion resistance, high ductility and high strength, mainly used for inner and outer panels of automobiles, and a method of manufacturing the same. The high-manganese hot-dip coated steel sheet includes a substrate steel sheet having a composition of (in weight %) 0.1 to 1.5% of C, 5 to 35% of Mn, and the remainder includes Fe and other unavoidable impurities, and a hot-dip zinc coating layer formed on the substrate steel sheet, the hot-dip zinc coating layer having a composition of (in weight %) 0.1 to 10% of Mn, 5 to 15% of Fe, and the remainder including Zn and other unavoidable impurities.

    摘要翻译: 的高锰热浸镀钢板是游离缺失盘,其提供高耐腐蚀性,高延性和高强度,主要用于汽车的内板和外板,及其制造方法。 的高锰热浸镀钢板包括具有的组成的基材钢板(重量%)C:0.1〜1.5%以下,Mn为5至35%,剩余部分包括Fe和其它不可避免的杂质,和一个 形成在基底钢板上的热浸镀锌层,其具有(以重量%计)0.1至10%的Mn,铁的5〜15%,剩余部分包含的Zn和其他的组合物的热浸镀锌层 杂质不可避免的。

    CRYOGENIC AUSTENITIC HIGH-MANGANESE STEEL HAVING EXCELLENT CORROSION RESISTANCE, AND MANUFACTURING METHOD THEREFOR

    公开(公告)号:EP3872212A1

    公开(公告)日:2021-09-01

    申请号:EP19875923.5

    申请日:2019-10-25

    申请人: POSCO

    摘要: The cryogenic austenitic high-manganese steel having excellent corrosion resistance, according to one aspect of the present invention, comprises 0.2-0.5 wt% of C, 23-28 wt% of Mn, 0.05-0.5 wt% of Si, 0.03 wt% or less of P, 0.005 wt% or less of S, 0.5 wt% or less of Al, and 3-4 wt% of Cr, with the remainder being Fe and other unavoidable impurities, also comprises at least 95 area% of austenite as a microstructure, and has Cr concentration sections continuously formed within an area of 50 µm in the thickness direction from the surface, wherein the Cr concentration sections comprise a high Cr concentration section having a relatively high concentration of Cr, and a low Cr concentration section having a relatively low concentration of Cr, and the high Cr concentration section may be distributed at 30 area% or less (but not 0%) relative to the whole surface area of the Cr sections.