公开(公告)号:EP2242585A4
公开(公告)日:2012-04-18
申请号:EP09700360
申请日:2009-01-09
发明人: SENIOR GEOFFREY DAVID , PYKE BRENDAN , JUDD BRIAN
IPC分类号: B03D1/02
CPC分类号: C22B1/00 , B03D1/002 , B03D1/02 , B03D2201/007 , B03D2203/02 , C22B23/005
-
公开(公告)号:EP2242586A4
公开(公告)日:2012-04-11
申请号:EP09700741
申请日:2009-01-09
发明人: SENIOR GEOFFERY DAVID , PYKE BRENDAN , JUDD BRIAN
IPC分类号: B03D1/02
-
公开(公告)号:EP2276865A4
公开(公告)日:2015-03-25
申请号:EP08865511
申请日:2008-12-24
CPC分类号: C22B23/005 , C22B3/42 , C22B3/44 , C22B23/0415 , C22B23/043 , C22B23/0453 , C22B23/0476 , Y02P10/234
摘要: A heap leach process for the recovery of nickel and cobalt from a lateritic ore, said process including the steps of leaching and/or agglomerating the ore with a lixiviant that includes ferrous ions, wherein the lixiviant is able to liberate cobalt from the cobalt containing minerals within the ore in preference to nickel, to produce a cobalt rich pregnant leach solution relatively free of nickel.
-
公开(公告)号:EP2285993A4
公开(公告)日:2014-09-10
申请号:EP09765249
申请日:2009-06-16
发明人: LIU HOUYUAN , ROCHE ERIC GIRVAN
CPC分类号: C22B23/0461 , C22B23/0415 , C22B23/043
-
公开(公告)号:EP2294232A4
公开(公告)日:2013-12-25
申请号:EP09768624
申请日:2009-06-25
发明人: ROCHE ERIC GIRVAN
CPC分类号: B01D9/004 , C22B3/44 , C22B23/0461 , Y02P10/234
摘要: A process for the treatment of a solution containing at least ferric ions, and one or more metal values, said process including the step of maintaining a controlled concentration of ferric ions in solution for a sufficient residence time to control iron hydroxide or oxide crystal growth, and precipitating the iron as a relatively crystalline iron hydroxide or oxide while minimising the loss of the ore or more metal values with the iron hydroxide or oxide.
-
公开(公告)号:EP2271780A4
公开(公告)日:2011-10-26
申请号:EP08864370
申请日:2008-12-24
发明人: MORONEY ADAM SEAN
CPC分类号: C22B23/043 , C22B23/0407 , C22B47/0063
-
公开(公告)号:EP1880029A4
公开(公告)日:2009-08-12
申请号:EP06721483
申请日:2006-05-11
发明人: LIU HOUYUAN
CPC分类号: C22B23/0423 , C22B1/243 , C22B23/005 , C22B23/043
摘要: A process for the recovery of nickel and cobalt from a nickeliferous oxidic ore by heap leaching, the process including the steps of: a) forming the nickeliferous oxidic ore into one or more heaps; b) leaching the ore heap with a leach solution in a leach step wherein the leach solution includes an acid supplemented hypersaline water as the lixiviant, the hypersaline water having a total dissolved solids concentration greater than 30 g/l; and c) recovering the nickel and cobalt from the resultant heap leachate.
-
公开(公告)号:EP2307582A4
公开(公告)日:2014-12-03
申请号:EP09802271
申请日:2009-07-29
发明人: DU PLESSIS CHRIS
IPC分类号: C22B3/06
CPC分类号: C22B3/06 , C22B3/08 , C22B3/18 , Y02P10/234
-
公开(公告)号:EP1971695A4
公开(公告)日:2009-12-16
申请号:EP06840395
申请日:2006-12-21
CPC分类号: C22B23/0461 , C01F5/40 , C22B23/043 , C22B26/22 , Y02P10/234
-
-
-
-
-
-
-
-