摘要:
An object of this invention is to provide a layered product of a non-polar rubber or a rubber having a small polarity which makes it difficult to bond the rubber with a different material and a different kind of rubber, which are stacked directly or via an adhesive layer, the layered product of this invention including at least one type of layer selected from the layers (1) and (2), and at least one type of layer selected from the layers (3) and (4), in which at least one layer of the at least one type of layer selected from the layers (1) and (2) is directly in contact with or adjacent via an adhesive layer to at least one layer of the at least one type of layer selected from the layers (3) and (4): layer (1): a layer prepared using an ethylene/α-olefin/non-conjugated polyene copolymer; layer (2): a layer prepared using an ethylene/carboxylic acid copolymer; layer (3) : a layer prepared using an acrylic-type rubber; and layer (4): a layer prepared using a halogen-containing polymer.
摘要:
The present invention relates to an elastic terpolymer that can acquire good mechanical properties and elasticity (flexibility) at the same time, and a preparation method thereof. The elastic terpolymer, which is a copolymer of 40 to 70 wt% of ethylene, 15 to 55 wt% of a C 3 -C 20 alpha-olefin, and 0.5 to 20 wt% of a diene as obtained in the presence of a group 4 transition metal catalyst, satisfies that: (i) the weight average molecular weight measured by GPC is 100,000 to 500,000; and (ii) the ethylene content x (wt%) and the crystallization enthalpy y (”HcJ/g) of the copolymer measured by DSC satisfy a defined relational expression.
摘要:
The invention provides a process to form an ethylene/α-olefin interpolymer, comprising at least the following steps A) through C): A) polymerizing, in at least one reactor, at least one reaction mixture comprising ethylene and the α-olefin, in a solution polymerization, and in the presence of at least the following components I), II) and III): I) at least one compound of Structure 1, as described herein; II) at least one co-catalyst, as described herein; III) at least one compound of Structure 2, as described herein; B) separating the final polymer solution into at least a polymer-rich solution and a polymer-free solution; and optionally, at least a portion of the polymer-free solution is recycled back to the reactor; C) maintaining the level of the at least one compound of Structure 2 in the at least one reactor, from 100 ppm to 10,000 ppm, as described herein.
摘要:
A railroad rail track pad composition including a particular ethylene·α-olefin·non-conjugated polyene random copolymer (A), clay (B), and a sulfur atom-containing silane coupling agent (C) is used in order to lower the viscosity of a rubber composition that is a raw material for molding while suppressing lowering of the rubber elasticity of a crosslinked and molded product to be obtained. In addition, a molded product obtained by crosslinking the composition, particularly a molded product obtained by crosslinking and foam-molding the composition, is provided with rubber elasticity that is suitable as a railroad rail track pad.