Abstract:
Methods for fabricating a capacitor are provided. In the methods, a dielectric may be formed on a metal (e.g. nickel) substrate, and a copper electrode is formed thereon, followed by the thinning of the metal substrate from its non-coated face, and subsequently forming a copper electrode on the thinned, non-coated face of the substrate.
Abstract:
An ionic polymer metal composite (IPMC) capacitor is disclosed which includes a thin single layer non-hydrated ionic polymer substrate with conductive film electrodes applied to at least a portion of each side of the non-hydrated ionic polymer substrate. The disclosed capacitor is suited for providing thin capacitance structures made to substantially any desired dimensions and shape and may be particularly suited for short term power storage in low power electronics, sensors, micro-electronics, MEMs and high temperature applications. A method of manufacturing an IPMC capacitor is also disclosed including providing a thin single layer non-hydrated ionic polymer substrate, applying a conductive film electrode to both sides of the substrate, and attaching electrical connections to the electrodes. The disclosed method of manufacture may optionally also include heat curing the capacitor and coating the capacitor with at least one moisture-resistant protective coating layer.
Abstract:
An ionic polymer metal composite (IPMC) capacitor is disclosed which includes a thin single layer non-hydrated ionic polymer substrate with conductive film electrodes applied to at least a portion of each side of the non-hydrated ionic polymer substrate. The disclosed capacitor is suited for providing thin capacitance structures made to substantially any desired dimensions and shape and may be particularly suited for short term power storage in low power electronics, sensors, micro-electronics, MEMs and high temperature applications. A method of manufacturing an IPMC capacitor is also disclosed including providing a thin single layer non-hydrated ionic polymer substrate, applying a conductive film electrode to both sides of the substrate, and attaching electrical connections to the electrodes. The disclosed method of manufacture may optionally also include heat curing the capacitor and coating the capacitor with at least one moisture-resistant protective coating layer.
Abstract:
A thin, rechargeable, flexible electrochemical energy cell includes a battery cell, or a capacitor cell, or a battery/capacitor hybrid cell that can be stackable in any number and order. The cell can be based on a powdery mixture of hydrated ruthenium oxide particles or nanoparticles with activated carbon particles or nanoparticles suspended in an electrolyte. The electrolyte may contain citric acid. An anode electrode may be formed with a thin layer of oxidizable metal (e.g., Pb). The cathode may be formed with a graphite backing foil. The materials used in the energy cell can be explosive-free, nonflammable, nontoxic, and environmentally safe, and the energy cell may have a voltage at or below 1.25V for recharging. The thickness of the cell structure can be in the range of 0.5 mm - 1 mm, or lower.