METHOD OF PRODUCING ADDITION PRODUCT OF COMPOUND CONTAINING SiH GROUP ONTO REACTANT HAVING ONE DOUBLE BOND IN AQUEOUS MEDIA
    83.
    发明专利
    METHOD OF PRODUCING ADDITION PRODUCT OF COMPOUND CONTAINING SiH GROUP ONTO REACTANT HAVING ONE DOUBLE BOND IN AQUEOUS MEDIA 有权
    生产含SiH组合物的添加剂产品的方法在具有水性介质中的双重粘结剂的反应物

    公开(公告)号:JP2007063554A

    公开(公告)日:2007-03-15

    申请号:JP2006222397

    申请日:2006-08-17

    CPC分类号: C08G77/38 C08G77/06 C08G77/46

    摘要: PROBLEM TO BE SOLVED: To provide a method of producing addition product of a compound containing SiH group onto a reactant having one double bond in an aqueous media.
    SOLUTION: The invention relates to the method of producing organically modified siloxanes and silanes by noble-metal-catalyzed reaction of siloxanes and/or silanes having at least one SiH group with a compound having one double bond, wherein the reaction is carried out in the presence of water as a reaction medium. The organically modified siloxanes and/or silanes obtained by the reaction are useful for a compound for detergent, an additive for dispersing in producing paint, foam stabilizer for polyurethane foam, textile treating agents, etc.
    COPYRIGHT: (C)2007,JPO&INPIT

    摘要翻译: 待解决的问题:提供一种在含水介质中在含有一个双键的反应物上生产含有SiH基团的化合物的加成产物的方法。 解决方案:本发明涉及通过具有至少一个SiH基团的硅氧烷和/或硅烷与具有一个双键的化合物的贵金属催化反应来生产有机改性的硅氧烷和硅烷的方法,其中反应进行 在作为反应介质的水的存在下。 通过该反应获得的有机改性的硅氧烷和/或硅烷可用于洗涤剂用化合物,用于分散制备涂料的添加剂,用于聚氨酯泡沫的泡沫稳定剂,纺织品处理剂等。版权所有(C)2007, JPO&INPIT

    CURABLE COMPOSITION
    84.
    发明专利
    CURABLE COMPOSITION 审中-公开

    公开(公告)号:JP2006348209A

    公开(公告)日:2006-12-28

    申请号:JP2005177553

    申请日:2005-06-17

    申请人: KANEKA CORP

    IPC分类号: C08G65/336 C08G77/46 C09K3/10

    摘要: PROBLEM TO BE SOLVED: To provide a curable composition useful as a sealant or an adhesive having excellent restoring properties, heat resistance and follow-up properties to movement of a joint over a long period and properties of following to an adherend and bonding thereto. SOLUTION: The curable composition comprises a polyoxyalkylene polymer (A). Furthermore, the polyoxyalkylene polymer (A) has 16,500-50,000 number-average molecular weight and contains a group represented by general formula (1) -(SiR 1 2 O) n SiR 1 2 -R 2 -SiX 3 (wherein, R 1 represents a monovalent hydrocarbon group and 2n+2 R 1 s may mutually be the same or different; R 2 represents a 1-20C bivalent hydrocarbon group; X represents a hydroxy group or a hydrolyzable group and 3 Xs may mutually be the same or different; and n represents an integer of 0-100) as a silicon-containing group cross-linkable by forming a siloxane bond. COPYRIGHT: (C)2007,JPO&INPIT

    Powder dispersion stabilizer and powder dispersion composition with the powder dispersion stabilizer incorporated therein
    86.
    发明专利
    Powder dispersion stabilizer and powder dispersion composition with the powder dispersion stabilizer incorporated therein 有权
    粉末分散稳定剂和粉末分散组合物与粉末分散稳定剂

    公开(公告)号:JP2006218472A

    公开(公告)日:2006-08-24

    申请号:JP2005352829

    申请日:2005-12-07

    摘要: PROBLEM TO BE SOLVED: To provide a novel powder dispersion stabilizer and a powder dispersion composition having excellent dispersion stability.
    SOLUTION: This powder dispersion stabilizer comprises a two-end silicone modified glycerin represented by general formula (a). The powder dispersion composition comprises the powder dispersion stabilizer incorporated therein. In formula (a), R1 represents a straight chain or branched alkyl group having 1 to 12 carbon atoms, or a phenyl group; R2 represents an alkylene group having 2 to 11 carbon atoms; m is 10 to 120; and n is 1 to 11.
    COPYRIGHT: (C)2006,JPO&NCIPI

    摘要翻译: 要解决的问题:提供具有优异的分散稳定性的新型粉末分散稳定剂和粉末分散组合物。 解决方案:该粉末分散稳定剂包含由通式(a)表示的二端硅氧烷改性甘油。 粉末分散体组合物包含掺入其中的粉末分散稳定剂。 式(a)中,R 1表示碳原子数1〜12的直链或支链烷基或苯基; R2表示碳原子数2〜11的亚烷基。 m为10〜120; n为1〜11。(C)2006,JPO&NCIPI

    Fixing device and image forming apparatus
    87.
    发明专利
    Fixing device and image forming apparatus 审中-公开
    固定装置和图像形成装置

    公开(公告)号:JP2006113132A

    公开(公告)日:2006-04-27

    申请号:JP2004297918

    申请日:2004-10-12

    IPC分类号: G03G15/20 C08G77/46

    摘要: PROBLEM TO BE SOLVED: To provide a fixing device for increasing the durability of a peeling member and for improving the image quality of a fixed image, and to provide an image forming apparatus equipped with the fixing device. SOLUTION: The fixing device comprises a fixing roller with a heat source, a pressure roller which is brought into pressure contact with the fixing roller, and a peeling member disposed near the fixing roller in the axial direction of the fixing roller and on a downstream side of a recording medium transport direction of a fixing nip portion. The peeling member comprises a substrate with a finely roughened surface and a coat disposed on the surface side of the substrate, wherein the substrate has a surface roughness Ra of 0.1-1.0 μm and a surface roughness Rz of 1.0-9.0 μm, and the coat is formed of a material, containing a hydrolytic condensation product of a silicon-containing compound represented by Formula (I). COPYRIGHT: (C)2006,JPO&NCIPI

    摘要翻译: 要解决的问题:提供一种用于提高剥离部件的耐久性并提高固定图像的图像质量的定影装置,并提供配备有定影装置的图像形成装置。 解决方案:定影装置包括具有热源的定影辊,与定影辊压力接触的压力辊和沿着定影辊的轴向方向设置在定影辊附近的剥离构件, 定影夹持部的记录介质输送方向的下游侧。 剥离部件包括具有细粗糙表面的基板和设置在基板的表面侧上的涂层,其中基板的表面粗糙度Ra为0.1-1.0μm,表面粗糙度Rz为1.0-9.0μm,涂层 由含有由式(I)表示的含硅化合物的水解缩合产物的材料形成。 版权所有(C)2006,JPO&NCIPI

    Composition for forming film, method for forming film, and silica-based film
    90.
    发明专利
    Composition for forming film, method for forming film, and silica-based film 审中-公开
    形成膜的组合物,形成膜的方法和基于硅胶的膜

    公开(公告)号:JP2005120355A

    公开(公告)日:2005-05-12

    申请号:JP2004273469

    申请日:2004-09-21

    摘要: PROBLEM TO BE SOLVED: To provide a composition for forming a film which can form a film having a low relative dielectric constant and exhibiting excellent chemical resistance. SOLUTION: The composition for forming the film comprises a hydrolyzate condensate (I) obtained by hydrolytically condensing (A) at least one silane compound, selected from among a compound (A-1) represented by general formula (1): R a Si(OR 1 ) 4-a , a compound (A-2) represented by general formula (2): Si(OR 2 ) 4 and a compound (A-3) represented by general formula (3): R 3 b (R 4 O) 3-b Si-(R 7 ) d -Si(OR 5 ) 3-c R 6 c , and (B) a cyclic silane compound represented by general formula (4), a compound (II) which is compatible with or dispersible in the hydrolyzate condensate (I) and has a boiling point or a decomposition temperature of 200-400°C, and an organic solvent (III). COPYRIGHT: (C)2005,JPO&NCIPI

    摘要翻译: 解决的问题:提供一种能够形成具有低相对介电常数并且具有优异的耐化学性的膜的薄膜形成用组合物。 解决方案:用于形成膜的组合物包含通过水解缩合(A)至少一种选自通式(1)表示的化合物(A-1)中的至少一种硅烷化合物获得的水解产物缩合物(I):R 通式(2)表示的化合物(A-2):Si(OR 1) SP> 2 )和通式(3)表示的化合物(A-3):R 3 b [R 4 O) 3-b SI-(R 7 ð -Si(OR 5 (B)由通式(4)表示的环状硅烷化合物,(b)由通式(4)表示的环状硅烷化合物, 与水解缩合物(I)相容或分散并具有200-400℃的沸点或分解温度的化合物(II)和有机溶剂(III)。 版权所有(C)2005,JPO&NCIPI