강관 파이프 인발장치
    41.
    发明公开
    강관 파이프 인발장치 无效
    绘制钢管的装置

    公开(公告)号:KR1020100019017A

    公开(公告)日:2010-02-18

    申请号:KR1020080077825

    申请日:2008-08-08

    申请人: 정임근

    发明人: 정임근

    IPC分类号: B21C1/06 B21C1/00

    摘要: PURPOSE: An apparatus for drawing a steel pipe is provided to manufacture a steel pipe of high quality, lower inferiority rate, and improve productivity by converting individual processes into a uniform automated process. CONSTITUTION: An apparatus for drawing a steel pipe comprises followings. A transfer table(20) consecutively guides the movement of a steel pipe(21). A dice block(22) which is equipped with a plug drawing out the steel pipe is installed on the transfer table. A drive guide is installed on the transfer table(23). A pulling bogie(25) contains a pipe clamper which is drawn out from the die block. A hydraulic cylinder is coupled by the pulling bogie and a rod(26) to move the pulling bogie along a drive guide(27).

    摘要翻译: 目的:提供一种用于拉制钢管的设备,通过将各个工艺转变为均匀的自动化工艺来制造高品质,低劣率的钢管,并提高生产率。 构成:用于拉制钢管的装置包括以下。 转台(20)连续引导钢管(21)的移动。 配备有拔出钢管的插头的骰子块(22)安装在转台上。 传动导轨安装在传送台(23)上。 拉动转向架(25)包含从模具块拉出的管夹持器。 液压缸通过牵引转向架和杆(26)联接,以沿着驱动引导件(27)移动牵引转向架。

    알루미늄 압착 선재피복장치와 이를 이용한 알루미늄 피복철망
    42.
    发明授权
    알루미늄 압착 선재피복장치와 이를 이용한 알루미늄 피복철망 有权
    铝用于线和铝包层网的压力覆盖装置

    公开(公告)号:KR100936541B1

    公开(公告)日:2010-01-13

    申请号:KR1020070117799

    申请日:2007-11-19

    申请人: 김종식

    发明人: 김종식

    摘要: 본 발명은 알루미늄 압착 선재피복장치와 이를 이용한 알루미늄 피복철망에 관한 것으로서, 상기 금속선재를 예열하는 예열기와, 알루미늄밴드가 권취된 알루미늄밴드릴과, 상기 알루미늄밴드릴로부터 인출되는 상기 알루미늄밴드를 원통형상으로 포밍하는 포밍부와, 상기 포밍된 알루미늄밴드의 접선부위를 용접하는 제1용접기와, 상기 금속선재의 외주면에 상기 포밍된 알루미늄밴드를 압착시키는 압착부와, 상기 알루미늄밴드가 압착된 알루미늄피복선재를 인출하는 인출부를 포함하되, 상기 포밍부는 상기 알루미늄밴드릴로부터 인출된 상기 알루미늄밴드를 만곡성형하는 만곡부와, 상기 만곡성형된 알루미늄밴드를 원통형상으로 유지하는 원통형상유지부를 포함하는 것을 특징으로 하는 알루미늄 압착 선재피복장치를 제공한다.
    상기와 같은 본 발명에 따르면, 알루미늄 압출기를 대신하여 포밍부와 압착부를 설치함으로써 설비 단가가 저렴하여 제조원가를 현저하게 절감할 수 있는 효과가 있다.
    또한, 용융도금로에 비해 설치공간의 제약이 적고, 알루미늄을 피복하는 구간이 짧아 제조시간이 줄어들게 되어 생산성이 향상되는 효과가 있다.
    피복, 권취, 포밍, 용접, 압착, 인출, 용융도금로

    결속용 철사의 제조 방법
    43.
    发明授权
    결속용 철사의 제조 방법 失效
    绑线的制造工艺

    公开(公告)号:KR100925222B1

    公开(公告)日:2009-11-06

    申请号:KR1020080018735

    申请日:2008-02-29

    发明人: 신용철

    摘要: 본 발명은 조선소 등에서 사용하는 결속용 철사의 제조방법에 관한 것으로, 철사의 인장 강도를 높이고 표면에서 녹 스는 것을 억제하기 위하여, φ5~6mm의 연강선재를 선택하는 선택공정과, 선택된 선재를 냉간 인발 공정에 의해 φ1~5mm의 선재로 만드는 인발 공정과, 인발된 선재를 700~750℃의 분위기에서 1~2시간 소둔 열처리하는 공정과, 열처리 된 선재를 소정의 길이로 절단하는 공정과, 절단된 선재의 표면을 코팅처리하고 건조하는 공정에 따라 결속용 철사를 제조하는 기술이다.
    철사, 결속, 열처리, 녹 방지, 코팅, 인발

    결속용 철사의 제조 방법
    44.
    发明公开
    결속용 철사의 제조 방법 失效
    绑线的制造工艺

    公开(公告)号:KR1020090093290A

    公开(公告)日:2009-09-02

    申请号:KR1020080018735

    申请日:2008-02-29

    发明人: 신용철

    摘要: A manufacturing method of a fastening wire is provided to identify a user of the fastening wire by marking at one part and to prevent the rust on the wire surface in the constructing of a ship. A manufacturing method of a fastening wire is as follows. The soft steel wire of Phi 5~6mm is selected. The selected wire is manufactured with the wire of Phi 1~5mm with a cold drawing process. The drown steel is heat treated at 700~750°C for 1~2 hours. The heat-treated wire is cut in the predetermined length. The surface of the cut wire is put on the coating solution of the synthetic resin class to be coated. The surface of the coated wire is dried with the hot air more than 20°C. One side of the coated wire is dipped in a paint tank to be marked. After the marked wire is divided and packed per a unit to be shipped out.

    摘要翻译: 提供紧固线的制造方法,以通过在一部分处标记来识别紧固线的使用者,并且防止在构造船舶时在线表面上的锈蚀。 紧固线的制造方法如下。 选择Phi 5〜6mm的软钢丝。 所选择的线材采用Phi 1〜5mm的线材进行冷拉加工。 淹钢在700〜750℃下热处理1〜2小时。 热处理的线材以预定长度切割。 将切割的线的表面放在要涂覆的合成树脂类的涂布溶液上。 涂覆线的表面用热空气干燥20多摄氏度。 将涂覆线的一侧浸入油漆罐中进行标记。 标记的电线每一个单元分开包装后运出。

    인서트용 강철봉 및 그 제조 방법
    45.
    发明授权
    인서트용 강철봉 및 그 제조 방법 有权
    插入钢棒及其方法

    公开(公告)号:KR100877240B1

    公开(公告)日:2009-01-07

    申请号:KR1020070055652

    申请日:2007-06-07

    申请人: 선상희

    发明人: 선상희

    IPC分类号: B21C1/00 B21C3/02

    摘要: 본 발명은 인서트(insert)용 강철봉 제조 방법에 관한 것으로서, (a) 그 일단의 직경이 전체 직경보다 작은 소정 길이의 강철봉을 준비하는 단계; (b) 강철봉의 일단을 내주면에 다수의 절삭팁이 방사상으로 형성된 내부 금형의 입구측으로 삽입하는 단계; 및 (c) 상기 내부 금형의 끝단으로부터 점차적으로 연장되며, 내부 금형의 반경보다 더 큰 반경을 가진 외부 금형의 출구측을 통해 강철봉을 뽑아냄으로써 상기 강철봉의 길이 방향으로 다수의 홈을 형성시키는 단계;를 포함하는 것을 특징으로 하는 인서트(insert)용 강철봉 제조 방법.

    인서트용 강철봉 및 그 제조 방법
    46.
    发明公开
    인서트용 강철봉 및 그 제조 방법 有权
    INSERT-STEEL ROD及其方法

    公开(公告)号:KR1020080107647A

    公开(公告)日:2008-12-11

    申请号:KR1020070055652

    申请日:2007-06-07

    申请人: 선상희

    发明人: 선상희

    IPC分类号: B21C1/00 B21C3/02

    摘要: An eyebar for insert and a manufacturing method using the same are provided as the product having the quality which is the eyebar for the insert of the semi-finished product form uniform. An eyebar(1) manufacturing method for the insert performs the followings: a step for preparing the eyebar of the fixed length in which the diameter of the one end is smaller than the whole diameter; a plurality of segments in the inner circumference is a step for inserting to the inlet of the radially formed inner mold one end of eyebar; the eyebar is extracted through the outlet side of the outside mold(20) having the radius which is bigger than the radius of the inner mold; and a step formed is characterized to the longitudinal direction of eyebar.

    摘要翻译: 提供了用于插入物的眼杆和使用其的制造方法作为具有作为半成品形状的插入物的均匀性的眼杆的品质的产品。 用于插入物的眼杆(1)制造方法执行以下步骤:制备其一端的直径小于整个直径的固定长度的眼杆的步骤; 在内圆周上的多个段是用于插入到径向形成的内模的入口的步骤,一个眼睑的一端; 通过具有大于内模半径的半径的外模20的出口侧抽出眼杆; 并且形成的台阶的特征在于眼杆的纵向。

    초고강도 스틸코드용 강선의 제조방법
    47.
    发明公开
    초고강도 스틸코드용 강선의 제조방법 有权
    生产超高强度钢丝的钢丝

    公开(公告)号:KR1020080073842A

    公开(公告)日:2008-08-12

    申请号:KR1020070012547

    申请日:2007-02-07

    发明人: 이충열 김민안

    CPC分类号: B21C1/003 C22C38/04

    摘要: A method for manufacturing a steel wire for a super high tenacity steel cord is provided to limit delamination, and to reduce the dice use and dice reduction by optimizing an approach angle of a dice which is installed in a wet wire draw bench, a dice tip material, and the dice reduction per a unit. A steel cord is manufactured by a hot rolled steel in which carbon content is 0.90 to 0.97 wt%, chrome content is 0.10 to 0.40 wt%, and a diameter is 5.5mm. A super high tenacity steel cord has a diameter of 0.1 to 0.4 mm and tensile strength of 360 to 420kg/mm^2. The super high tenacity steel cord is drawn by passing the steel cord through a dice which is installed in a wet wire draw bench. An approach angle of a dice tip installed in the wet wire draw bench is 7 to 9°. A dice reduction per an initial deformation section unit is 8 to 13%, a dice reduction per a middle deformation section unit is 14 to 17%, and a dice reduction per an end deformation section unit is 13 to 14% by using the dice in which cobalt content of the dice tip is 2 to 4 weight%.

    摘要翻译: 提供了一种用于制造用于超高强度钢丝帘线的钢丝绳的方法,以限制分层,并且通过优化安装在湿拉丝台上的骰子的接近角度来减少骰子使用和骰子减少,骰子尖端 材料和每个单位的骰子减少量。 钢丝帘线由碳含量为0.90〜0.97重量%,铬含量为0.10〜0.40重量%,直径为5.5毫米的热轧钢制成。 超强韧钢丝绳的直径为0.1〜0.4mm,拉伸强度为360〜420kg / mm ^ 2。 超高强度钢丝绳通过将钢丝绳穿过安装在湿拉丝台上的骰子来拉伸。 湿式拉丝台中安装的骰子尖的接近角为7°至9°。 每个初始变形部分单元的骰子减少量为8至13%,每个中间变形部分单元的骰子减少量为14至17%,并且通过使用骰子在每个端部变形部分单元中的骰子减少量为13至14% 骰子尖端的钴含量为2〜4重量%。

    차량용 랙튜브의 인발 성형장치 및 방법
    48.
    发明授权
    차량용 랙튜브의 인발 성형장치 및 방법 有权
    汽车机架的推进机及其方法

    公开(公告)号:KR100778526B1

    公开(公告)日:2007-11-22

    申请号:KR1020060089333

    申请日:2006-09-14

    申请人: 태림산업(주)

    发明人: 오승한

    摘要: A draw shaping apparatus and method of a rack-tube for a vehicle are provided to improve productivity by processing the production of rack bush automatically and by performing loading and drawing simultaneously. A draw shaping apparatus for a vehicle comprises a loading unit for loading an inserted workpiece one by one, a moving unit provided in one side of the loading unit and supporting the workpiece transferred by the loading unit, an up and down moving unit provided in one side of the moving unit and controlling up and down movement of the moving unit, a back and forth moving unit provided in one side of the moving unit and controlling back and forth movement of the moving unit, a mold unit(150) for holding the workpiece transferred by the moving units and supporting draw shaping of a rack-tube, a press unit(160) for inserting the workpiece inside the press unit and pressing the workpiece, and a drawing unit(170) for extracting the rack-tube draw shaped inside the press unit out of the press unit.

    摘要翻译: 提供一种用于车辆的齿条管的拉伸成形设备和方法,以通过自动地进行齿条衬套的生产并且同时进行加载和拉伸来提高生产率。 一种用于车辆的牵伸成型装置,包括:一个一个地装载插入的工件的装载单元;设置在装载单元的一侧并支撑由装载单元传送的工件的移动单元;一个设置在一个中的上下运动单元 移动单元的一侧,并且控制移动单元的上下移动,设置在移动单元的一侧中的前后移动单元,并且控制移动单元的前后运动;模具单元(150),用于保持 由移动单元传送的工件和支撑架的成形,用于将工件插入压制单元内并按压工件的压制单元(160),以及用于抽出齿条管拉伸成形的拉伸单元(170) 在印刷机内部出现印刷机。

    냉간압조용 강선
    49.
    发明授权
    냉간압조용 강선 有权
    冷锻钢丝

    公开(公告)号:KR100568058B1

    公开(公告)日:2006-04-07

    申请号:KR1020030049957

    申请日:2003-07-21

    申请人: 삼화스틸(주)

    发明人: 안순태

    IPC分类号: B21C1/00

    摘要: 본 발명은 비교적 높은 강도가 요구되는 기계구조용 부품으로서의 각종 볼트류와 샤프트 등의 소재로 사용되는 강선 또는 강봉에 관한 것이다.
    본 발명은 C 0.10 ∼ 0.40wt%, Si 1.0wt% 이하, Mn 0.30 ∼ 2.0wt%, P 0.03wt% 이하, S 0.03wt% 이하가 함유되고 잔부가 Fe와 불가피한 불순물로 이루어지며 인장강도 70 ∼130Kgf/㎟로 칭, 템퍼링 열처리된 강선으로서 인장강도(TS)에 대한 단면감소율(δ,%)의 비(δ/TS)가 0.4 ∼ 1.2 인 것을 특징으로 하는 냉간압조 특성이 우수한 칭, 템퍼링 열처리된 강선을 제공한다.
    본 발명에 의하면, 강선의 제조 회사는 장시간의 구상화 소둔가열이 필요없게 되며 고주파유도 가열방식에 의한 단시간의 칭,템퍼링처리로서 구상화소둔과 동등하거나 그 이상의 압조가공성을 가지는 조질강선을 제조할 수 있으므로 생산성이 향상된다.

    냉공조용 파이프의 성형 방법
    50.
    发明公开
    냉공조용 파이프의 성형 방법 无效
    形成空调管的方法

    公开(公告)号:KR1020020094579A

    公开(公告)日:2002-12-18

    申请号:KR1020010032855

    申请日:2001-06-12

    申请人: 김갑영

    发明人: 김갑영

    IPC分类号: B21C1/00

    摘要: PURPOSE: A method for forming an air conditioning pipe is provided to reduce the time and processes for forming by forming an air conditioning pipe through the drawing work and to form a straight small hole in the center of a brass pipe. CONSTITUTION: A first and a second empty materials(10,20) are prepared. The first material is inserted to a hole of the second material. One end portion of the second material is processed by the pointing work. Then, a processed face(30) is formed. The processed face is fixed on a dice(50). A small hole is formed in the processed face by the drawing work.

    摘要翻译: 目的:提供一种用于形成空调管的方法,以通过在拉拔作业中形成空调管而缩短形成时间和工序,并在黄铜管的中心形成直的小孔。 规定:准备第一个和第二个空的材料(10,20)。 第一材料插入到第二材料的孔中。 第二材料的一个端部通过指示工作进行处理。 然后,形成加工面(30)。 经处理的面固定在骰子(50)上。 在加工面上通过拉拔加工形成小孔。