흡착제 조성물 및 이의 제조 방법
    59.
    发明公开
    흡착제 조성물 및 이의 제조 방법 无效
    吸附组合物及其制备方法

    公开(公告)号:KR1020120087018A

    公开(公告)日:2012-08-06

    申请号:KR1020110008448

    申请日:2011-01-27

    摘要: PURPOSE: An absorbent composition and a method for manufacturing the same are provided to prevent the generation of secondary environmental pollution and to reduce the escaping rate of particles from an oil fence. CONSTITUTION: A porous inorganic absorbent composition includes micro mixtures composed of 35 to 42 weight% of illite, 30 to 40 weight% of tourmaline, 9 to 20 weight% of mordenite, and 4 to 12 weight% of monazite. The average particle diameter of the micro mixtures is between 1 and 5um. The illite, the tourmaline, the mordenite, and the monazite are thermally treated for 10 minutes or more respectively at a temperature between 950 and 1000 degrees Celsius, 750 and 850 degrees Celsius, 750 and 850 degrees Celsius, and 600 and 700 degrees Celsius.

    摘要翻译: 目的:提供一种吸收剂组合物及其制造方法,以防止产生二次环境污染并降低颗粒从油栅栏中逸出的速度。 构成:多孔无机吸收剂组合物包括由35至42重量%的伊利石,30至40重量%的电气石,9至20重量%的丝光沸石和4至12重量%的独居石组成的微混合物。 微混合物的平均粒径为1-5微米。 分别在950-1000摄氏度,750摄氏度,850摄氏度,750摄氏度,850摄氏度,以及600摄氏度和700摄氏度之间,分别对伊利石,电气石,丝光沸石,独居石进行10分钟以上的热处理。