公开(公告)号:US06830604B2
公开(公告)日:2004-12-14
申请号:US10278073
申请日:2002-10-23
申请人: Alistair Grearson , John Aucote
发明人: Alistair Grearson , John Aucote
IPC分类号: C22C110
CPC分类号: C22C29/08
摘要: A dense cemented carbide product is described. The product is manufactured from WC with a grain size between 0.1 and 0.4 &mgr;m, fine grain size cobalt and ruthenium powders. The product is used in PCB machining operations where the addition of 10-25% Ru to the binder phase offers up to 25% wear resistant increases and up to 100% increase in chipping resistance in PCB routing compared to conventional materials (6% cobalt and 0.4 &mgr;m grain size).
摘要翻译: 描述了一种致密的硬质合金产品。 该产品由粒径在0.1和0.4μm之间的WC制成,细粒度的钴和钌粉末制成。 该产品用于PCB加工操作,其中与常规材料相比,粘合剂相中添加10-25%Ru可提供高达25%的耐磨性增加和PCB布线抗折叠性能提高100%(6%的钴和 0.4粒子粒径)。
-
公开(公告)号:US06521172B2
公开(公告)日:2003-02-18
申请号:US09486586
申请日:2000-05-15
申请人: Alistair Grearson , John Aucote
发明人: Alistair Grearson , John Aucote
IPC分类号: C22C3200
CPC分类号: C22C29/08
摘要: A dense cemented carbide product is described. The product is manufactured from WC with a grain size between 0.1 and 0.4 ¼ m, fine grain size cobalt and ruthenium powders. The product is used in PCB machining operations where the addition of 10-25% Ru to the binder phase offers up to 25% wear resistant incrases and up to 100% increase in chipping resistance in PCB routing compared to conventional materials (6% cobalt and 0.4 ¼ m grain size).
摘要翻译: 描述了一种致密的硬质合金产品。 该产品由粒径为0.1至0.4微米的WC制成,细粒度的钴和钌粉末制成。 该产品用于PCB加工操作,其中与常规材料相比,粘合剂相中添加10-25%Ru可提供高达25%的耐磨性和PCB布线抗折叠性能提高100%(6%的钴和 0.4μm粒度)。
-
公开(公告)号:US06413293B1
公开(公告)日:2002-07-02
申请号:US09486603
申请日:2000-08-16
IPC分类号: C22C2900
CPC分类号: C22C29/08
摘要: The present invention relates to a method of making ultrafine WC—Co alloys from a well dispersed mixture of fine and non-agglomerated WC and Co powders, wherein the Co powders have a narrow grain size distribution wherein at least 80% of the grains have sizes in the interval x+0.2x with the interval of variation of 0.4x is not smaller than 0.1 um, and a carbon content of approximately the amount necessary to provide eta phase formation.
摘要翻译: 本发明涉及从精细和非聚集的WC和Co粉末的良好分散的混合物制备超细WC-Co合金的方法,其中Co粉末具有窄的晶粒尺寸分布,其中至少80%的晶粒具有尺寸 间隔x + 0.2x,变化间隔为0.4x的间隔不小于0.1um,碳含量约为提供η相形成所需的量。
-
-