摘要: A polyvinylacetal resin powder with a low metal content, being excellent in transparency, moisture resistance and electrical insulating properties and having a large specific surface area, and a process for its production, are presented. A polyvinylacetal resin powder obtained by reacting polyvinyl alcohol and an aldehyde in the presence of an acid catalyst, which has an acetalization degree of at least 60 mol %, a specific surface area of from 1.50 to 3.50 m2/g, a bulk density of from 0.12 to 0.19 g/cm3, an average particle diameter of from 0.5 to 2, 5 μm and a metal content of at most 80 ppm.It is produced, for example, by feeding a reaction fluid containing polyvinyl alcohol, an aldehyde and an acid catalyst into a first reactor, to carry out an acetalization reaction, discharging the reaction fluid wherein the acetalization degree has reached from 10 to 60 mol %, and feeding the same into a second reactor to carry out a further reaction to bring the acetalization degree of polyvinylacetal to at least 65 mol %.
摘要翻译: 本发明提供一种金属含量低的聚乙烯醇缩醛树脂粉末,其透明性,耐湿性,电绝缘性优异,比表面积大,其制造方法。 在酸催化剂存在下,使聚乙烯醇与醛反应得到的聚乙烯醇缩醛树脂粉末,其缩醛度为至少60摩尔%,比表面积为1.50〜3.50m 2 / / g,堆积密度为0.12〜0.19g / cm 3,平均粒径为0.5〜2.5μm,金属含量为80ppm以下。 例如,通过将含有聚乙烯醇,醛和酸催化剂的反应流体供给到第一反应器中进行缩醛化反应,将缩醛化度达到10〜60摩尔%的反应液排出, 并将其进料到第二反应器中进行进一步的反应,使聚乙烯醇缩醛的缩醛化度达到至少65mol%。
-
公开(公告)号:US20050159545A1
公开(公告)日:2005-07-21
申请号:US10503123
申请日:2003-02-07
申请人: Yoshihiro Mashiko , Toshiaki Kawanishi , Koichi Matsunaga , Manabu Tsuzuki , Kazumasa Matsuoto , Koki Goto , Hitoshi Watanabe
发明人: Yoshihiro Mashiko , Toshiaki Kawanishi , Koichi Matsunaga , Manabu Tsuzuki , Kazumasa Matsuoto , Koki Goto , Hitoshi Watanabe
IPC分类号: C08F8/28 , C08F16/38 , C09D129/14 , C08F8/00
CPC分类号: C09D129/14 , C08F8/48 , C08F16/38 , C08F8/28 , C08F16/06
摘要: A polyvinylacetal resin powder with a low metal content, being excellent in transparency, moisture resistance and electrical insulating properties and having a large specific surface area, and a process for its production, are presented. A polyvinylacetal resin powder obtained by reacting polyvinyl alcohol and an aldehyde in the presence of an acid catalyst, which has an acetalization degree of at least 60 mol %, a specific surface area of from 1.50 to 3.50 m2/g, a bulk density of from 0.12 to 0.19 g/cm3, an average particle diameter of from 0.5 to 2, 5 μm and a metal content of at most 80 ppm. It is produced, for example, by feeding a reaction fluid containing polyvinyl alcohol, an aldehyde and an acid catalyst into a first reactor, to carry out an acetalization reaction, discharging the reaction fluid wherein the acetalization degree has reached from 10 to 60 mol %, and feeding the same into a second reactor to carry out a further reaction to bring the acetalization degree of polyvinylacetal to at least 65 mol %.
摘要翻译: 本发明提供一种金属含量低的聚乙烯醇缩醛树脂粉末,其透明性,耐湿性,电绝缘性优异,比表面积大,其制造方法。 在酸催化剂存在下,使聚乙烯醇与醛反应得到的聚乙烯醇缩醛树脂粉末,其缩醛度为至少60摩尔%,比表面积为1.50〜3.50m 2 / / g,堆积密度为0.12〜0.19g / cm 3,平均粒径为0.5〜2.5μm,金属含量为80ppm以下。 例如,通过将含有聚乙烯醇,醛和酸催化剂的反应流体供给到第一反应器中进行缩醛化反应,将缩醛化度达到10〜60摩尔%的反应液排出, 并将其进料到第二反应器中进行进一步的反应,使聚乙烯醇缩醛的缩醛化度达到至少65mol%。
-