公开(公告)号:US06808672B2
公开(公告)日:2004-10-26
申请号:US09940494
申请日:2001-08-29
申请人: Robert Michael Stewart , Chan Pak Kuen , Ralph Nicholas Spearman , Norhisham MD Sanusi , David William Fountain
发明人: Robert Michael Stewart , Chan Pak Kuen , Ralph Nicholas Spearman , Norhisham MD Sanusi , David William Fountain
IPC分类号: H05B664
CPC分类号: C08C1/14 , B29B13/06 , B29B13/08 , B29B15/04 , B29C35/045 , B29C2035/0855 , B29K2105/0064 , C08C3/00 , Y10S528/936
摘要: A process for the continuous coagulation and drying of rubber latex includes feeding the latex onto an endless conveyor belt which feeds the latex through a coagulator. A combination of microwave energy and hot air raises the temperature of the latex causing it to coagulate in a coagulation time of less than five minutes. The coagulated rubber from the coagulator is fed into a conveyor belt of a stretch unit which stretches the rubber by increasing its speed of travel. The stretched rubber is then conveyed onto the upper belt of a drying unit. The drying rubber is passed from the upper belt onto an intermediate belt and then on to a lower belt before leaving the drying unit. A combination of microwave energy and hot air in the drying unit is used to dry the rubber to a moisture content of less than 1.5%.
摘要翻译: 用于橡胶胶乳的连续凝结和干燥的方法包括将胶乳进料到通过凝结剂进料胶乳的循环传送带上。 微波能量和热空气的结合提高了胶乳的温度,使凝胶凝固时间少于5分钟。 来自凝结器的凝固橡胶被送入拉伸单元的输送带,拉伸单元通过增加其行进速度来拉伸橡胶。 然后将拉伸的橡胶输送到干燥单元的上部带上。 干燥橡胶在离开干燥单元之前从上部带传递到中间带上,然后到达较低的带。 使用干燥单元中的微波能量和热空气的组合来将橡胶干燥至小于1.5%的含水量。